morrisman
2nd Oct 2016, 05:28 PM
Many years ago, I made a new tailgate for my Land Rover . Its 1.2mm Aluminium stuck together with liquid nails . The original method was spot welding
I made a folder and dies .
364535
I made a folder and dies .