johnbaz
14th Aug 2016, 09:45 AM
Hi all
here's another Airsporter that needed a little tlc although I didn't reblue this one, I used coarse wire wool soaked in light machine oil, I couldn't believe the difference to the meatwork this made!!!
The stock was sunbleached to almost white so I had to strip it and then oil it, Couldn't believe the grain that surfaced!!
363814
363815
363816
363817
363818
363819
363820
363821
363822
I had this gun given as a freebie, I just had to pay postage as the gent was at the other end of the country!! Amazing it fired beautifully!!!
Regards, John :)
here's another Airsporter that needed a little tlc although I didn't reblue this one, I used coarse wire wool soaked in light machine oil, I couldn't believe the difference to the meatwork this made!!!
The stock was sunbleached to almost white so I had to strip it and then oil it, Couldn't believe the grain that surfaced!!
363814
363815
363816
363817
363818
363819
363820
363821
363822
I had this gun given as a freebie, I just had to pay postage as the gent was at the other end of the country!! Amazing it fired beautifully!!!
Regards, John :)