View Full Version : Opinon from experinced muzzle loader shooters sought ?
Grahame Collins
27th Jul 2015, 07:37 PM
I seek opinion specifically relating to muzzle loader and pulling a round ball.
After seeing someone nearly ruin a range rod trying to pull a double patched ball caught in built up barrel fouling, I have thought about a new way to achieve it with less chance of damaging a rod.
Typically range rods are made up from 6mm stainless rod. Sometimes they don't fare too well when some 125 Kilo gorilla tries to help another shooter with a jammed ball.
Generally what happens when it goes pear shaped, is that the ball and patch gets caught on barrel fouling if the ball is double patched.
The said gorilla, in ignorance and unable to pull the ball, hooks the rod handle in the roof beam of the shooting bay and hangs his weight on the rifle. Range rods get bent from this mis-treatment.
I thought there had to be an easier and safer way.
My thoughts are on making an 8mm diameter rod and using a type coach screw threaded to 10/32 UNF ( thats a standard cleaning rod thread) used for jags and brushes.
With a screw centering collar made from a flash machining plastic and the coach screw is less like to strip from the ball. The opposite end at the handle with be tapped to take a 400mm length of rod that takes a 2 kilo slide hammer cast from lead. What happens then is that slide hammer does its thing and pulls ball.The coarse pitched type 17 coach screw is less likely to strip through the lead ball. The force is axial to that of the barrel and should pull the ball with relative ease.
Simples?
What are your thoughts on the method and materials?
Non muzzle loader readers, please note that safety precautions are observed ie" percussion cap removed ,nipple removed and powder charge is oiled so the rifle can't accidentally discharge and shoot the gorilla.
Opinion will be appreciated.
Thanks
Grahame
barkersegg
27th Jul 2015, 08:56 PM
Grahame,
haven't done any ML for a while so this may be old hat, but I did make a rod tool such as you suggest out of brass rod and brazed a long self tapping metal screw into the end which I cut and trimmed to a short stubby length to try and pierce the lead pill - preferred the self tapper as the flutes cut more into the lead to hold it than a normal UNF. In those days I was only casting lead so hardness didn't matter but doubt it would be any good for a 20 or 30 to one brew. You then tried to screw the short stub thread into the ball but as you rightly suggest, the patches would invariably get mixed up and it was a nightmare. I often thought of getting a left handed thread tool inside a domed fitting to try and pierce the ball centrally - but it's not a problem screwing onto the ball, it's trying to initially move it by rotating it before trying to withdraw it....I know what a PITA it can be - might I suggest you have a look at one of the dedicated forums and post there such as www.castboolits.gunload.com (http://www.castboolits.gunload.com) - there are some knowledgeable folk there and I'm sure they'll have the answer......good luck whatever method you choose
ian
27th Jul 2015, 11:26 PM
not a muzzle loader but have a passing interest in muzzle loading naval canon
does the ball and patch get stuck during loading or on firing?
I understand that the tools used with a naval canon included a screw for extracting the ball if the canon wouldn't fire -- typically because the power became wet. Can see no reason why a similar tool wouldn't work with a muzzle loading rifle.
a quick google came up with ...
http://www.buffaloarms.com/Muzzleloader_Bullet_Puller_pr-5594.aspx?CAT=5594
Grahame Collins
28th Jul 2015, 12:02 AM
Cannons are swabbed after each shot to prevent left over embers from igniting the powder. I would imagine it was easy to misjudge the amount of "wet" to swab out with.
There is no patch in a cannon load as with a cap and ball m/loader rifle. The cloth patch acts as a gasket between ball and rifling.
Multiple shots with out cleaning between shots allow black powder fouling to build up which is further " hardened" by every subsequent shot.
If you clean with a "slighty" moist patch between shots, it provides excellent accuracy and minimises stuck ball and patch episodes on loading.
Mainly it is new comers that suffer from from stuck balls.
Causes are
A dirty bore
A double patch ball - pre damped patches can stick to each other and loaded if care is not taken
Patch used too thick.
Dry balling - loading a patched ball but forgetting the powder
If you spot a middle aged guy in a haberdashery store with a micrometer measuring cloth thickness - he is likely a muzzleloader.
Grahame
Grahame Collins
28th Jul 2015, 10:47 AM
Grahame,
but it's not a problem screwing onto the ball, it's trying to initially move it by rotating it before trying to withdraw it....I know what a PITA it can be -
The standard ball screws are to small and have a shallow pitch groove. The one in the pic is bigger. As far as the rotation - for following the rifling- I am building the rod with thrust bearing in the handle. I am not sure it it will stand up to the slide hammer impacts but don't see them as being all that much .It just needs to move the ball a tiny bit . Note the front of the screw it will self drill into the ball- Its on another range rod at the time photo was taken.
Also a pic of what a muzzle loader can do when it is shot clean. This is 54 cal at 25 meters. A string of 4 in the ten and one in the nine. (did not wipe the bore before I loaded that shot.)
barkersegg
28th Jul 2015, 01:52 PM
Grahame, that's about the thread shape of the screw I used but not as deep in the point..some old tools I have seen use a small cork screw type attachment but I think you'd run damaging the barrel because of it flexing and additionally with what hardness you cast.
I often thought the larger flaring of the screw may dig in deeper to get a firmer purchase but in experience found it made no difference because it wasn't so much the ball getting stuck but rather the patch as you said blocking anything from moving so half the time you never knew what you were in and just hoped it was tight enough....I think the most common mistake I made was in using excessive force first up to try and move the pill once I thought the screw had bit, it invariably tore out....so I don't know if your slide hammer idea would work any better ....can see where the idea of a threaded type pull of the rod causing a gradual force to extract it is probably the way to go or definitely worth a try but I never made anything like that or have seen similar used....don't think it would be too hard but then I was always loath to use steel rods as extraction tools in the bore anyway.
I read somewhere once about a process involving some form of solvent to dissolve any non metallic product first and allow easier extractions with the normal extraction screw bit but no doubt that was time restrictive and messy and not something you could do on at the bench....will see if I can find the link for you...sorry but have no other suggestions for you......good luck
barkersegg
30th Jul 2015, 02:47 PM
Grahame, have attached a couple of piccies to show the two different styles of worms that I was familiar with...I tried the make the second type single screw type but could never get any benefit over the earlier double cork screw type - these are available from Track of The Wold in the US but you'd no doubt be aware of them already...sorry haven't been much help
Grahame Collins
30th Jul 2015, 04:52 PM
barkersegg
Thanks so much for the pics pardner.
The long taper screw certainly looks like it has some promise. The corkscrew ones are lost patch removal tools and none work very well. As it happens I talked with a friend with a lot of Black powder firearm gunsmithing experience .
He showed me some patch pullers made from stainless steel fish hooks that mount on a piece of brass that work extremely well.
For pulling a ball he recommended pre drilling the ball and said the ball will come out real easy once drilled.It was essential ,he said, to have a insert to center the drill into the very middle of the ball.
There is nothing to it, in adding a small tap size drill to the kit. Hopefully I may have the opportunity to test it out on the week end as I am possibly going to the range. There always someone with a stuck ball,
I did a bit of searching on the American ML forums and found there was a tool called a - wait for it - Kadooty .
The Kadooty performed two functions- Firstly to tamp the powder load down to a consistent height and secondly to remove a jammed ball. Pictures showed a lost of rods that screw together and a sliding hammer - AKA a fairly small lump of brass maybe 25MM diameter.
It only stuck around a few years as there almost no mention of it now. As far as ordering over seas now I could n't be bothered as a relatively low priced item escalates in price once its had a boat ride to Australia. The way things are going we will have to make our own percussion caps as they are in very short suppy.
Thanks for the effort in digging up those pics.
Cheers
Grahame
bsrlee
30th Jul 2015, 10:34 PM
All these gadgets were standard fittings on a 'Sergeant's Tool' for the British Enfield 185x series of rifled muzzleloaders. There was a screw on tool with a spike, one with a fairly blunt, coarse threaded left hand screw and a two pronged screw - these all unscrewed from the ends of the 'Y' shaped tool and screwed onto the regular cleaning rod. The tool also included screwdrivers to fit all the screws, a main spring vice and a nipple prick. Dixie Gunworks may or may not still stock them.
GWH74
5th Mar 2016, 10:11 AM
Another option while very messy is to unscrew the nipple and screw in a grease fitting and push the balls out with grease.
I think I have also seen a device where you connect a CO2 inflator (like a bike tire one) and it blows the balls out using the C02.
Not sure if either these two methods will get a double ball out. Good for when you forget to add powder.
Grahame Collins
5th Mar 2016, 01:54 PM
Thanks GWH74,
If the devices are available herein Oz I don't know who has one .Forbes Agencies or Green River don't have them and basically they are the sellers of anything black powder orientated .
I have nearly perfected a slide hammer ball removal sytem. Still a bug or two to sort but I think it will work pretty good.
Cheers Grahame
eskimo
10th Mar 2016, 08:44 AM
A string of 4 in the ten and one in the nine.
a click or two right and and a few up ((or is that left and a few down ....did you shoot that on an upside target) they all would have been tens
A lot of service pistol shooters cant do that at 25 either....let alone 50
pretty good shooting Grahame
Grahame Collins
10th Mar 2016, 12:21 PM
a click or two right and and a few up ((or is that left and a few down ....did you shoot that on an upside target) they all would have been tens
A lot of service pistol shooters cant do that at 25 either....let alone 50
pretty good shooting Grahame
Some one wasn't looking when he put the targets up. The flyer was down to me not the rifle as I did not swab on the last shot. The rifle "fits" like it was made for me.
The rifle is without doubt the best I have ever shot . The particular rifle belongs to a mate who purchased it last year from Alan Vaisham at Green Rifle Rifle works in Adelaide.
It is basically hand assembled and fitted out by Alan. I think it rates with any custom produced muzzle loader rifle the yanks can produce. Sadly Alan Vaisham is retiring and won't be making any more of these wonderful guns.
Mate reckons it will be buried with him as he would never sell it. I told him OK I would come and dig it up.Talk about prying the gun from my cold dead hands.:D
Grahame
eskimo
10th Mar 2016, 12:38 PM
Sadly Alan Vaisham is retiring and won't be making any more of these wonderful guns.
his work will be missed
Hornetb
10th Mar 2016, 01:34 PM
I've seen the grease method and it works, it was used on a ball that was so boogered up from multiple attempts at screwing something into the ball that there was very little to tap into properly. So another thumbs up for that.
Messy, but if you've got your balls stuck. :oo:
Another option while very messy is to unscrew the nipple and screw in a grease fitting and push the balls out with grease.
I think I have also seen a device where you connect a CO2 inflator (like a bike tire one) and it blows the balls out using the C02.
Not sure if either these two methods will get a double ball out. Good for when you forget to add powder.
Grahame Collins
11th Mar 2016, 10:15 AM
The fact that neither Co2 removers and grease extraction methods are not on the dedicated Australian muzzle loading suppliers would indicate they are not in widespread use.
I have shot a lot of matches in a lot of places and am yet to see one. Maybe they are there in the southern states but none here in the north.
What I sought to do was make a simple tool that avoids the problems of other methods.
Mention was made of stripping the ball and that has been overcome by better hardware and technique
I have one being tested by some friends and currently waiting for feedback. When i have positive results from a range of different people I will post them.
Thanks for your replies
Grahame
Grahame Collins
27th Feb 2021, 01:46 PM
UPdate 2021
Finally!
I removed digit from rear end and got to building and finishing a stuck ball extractor tool. The 200 kg gorilla not needed.
It consists of :
An 8mm rod some 350mm longer than barrel with a crank at one end and thread connection the other
A cast weight that slides on the 8mm rod-52mm in diameter and 60mm long -used a small pasta sauce can as mould.
A screw to penetrate the round ball after the ball is drilled
A drill bit Small as the the screw minor diameter .
A spacer to center the drill and the screw in the center of the ball
When a stuck ball occurs remove nipple and flood the cavity with oil or water. To anyone who challenges the step to this point I will simply refer you to the Pedersoli instructions to remove a stuck ball.
Rod with drill and centering attached is fed down the barrel and handle cranked to drill ball.
Rod is removed and fitted with screw puller and sliding lead weight at crank end and rod is then cranked clockwise to thread through the stuck ball.
Also copiously oil the muzzle side of the ball to aid the sliding function.
A gentle slide and bump action removes the ball easily. It took easy 3 bumps to get the dry balled .54 cal ball sliding.
Disclaimer Please USE your own common sense and safe practice -no responsibility accepted. This way is very similar to the Pedersoli instructions for ball removal.
Note that this will not be allowed on SSAA controlled ranges as it contravenes the stuck round rules. I had to take my loaded muzzleloader OFF RANGE to free the ball.
At the same time Pedersoli (see their instructions on this ) has no problems using this system ( connected via a normal range rod) given that the powder is soaked and made ineffective by water and oil.
I hope it may be useful to someone.391008391009
Grahame Collins
17th Apr 2022, 04:52 PM
I've seen the grease method and it works, it was used on a ball that was so boogered up from multiple attempts at screwing something into the ball that there was very little to tap into properly. So another thumbs up for that.
Messy, but if you've got your balls stuck. :oo:
More update April 2022
I looked at making a grease gun system but you are correct -too messy.
The reason why the ball gets boogered is that the person removing the ball has not drilled the ball to take the screw which in turn is relative to the drill diameter in size.
Also it is important that the drill and the screw are centered reasonably other wise the rod deflects and the skews off to the side.
This is where it is different from other ball puller screw systems.
The Ball is drilled first-(on center) and then the screw- (a roof screw) - is tapped into the drilled - on center hole. Because the cranked handle unscrews-the slide hammer-can be then fitted after the hole drilling- it makes life a bit easier.
The slide hammer- lead cast into a small pasta tomato paste can is just the right weight to gently dislodge the ball. There plentiful oil on both sides of the ball and all it takes is a slight tap- a- tap to dislodge the ball
On average it is about 2 minutes work to free a ball. Having used it several times now all I can say the only disadvantage is the length of of pull rod which makes it a pain in the bum to case.
I am not keen on cutting it and threading it.
Maybe I might make a smaller diameter puller- but longer to better fit the carry case which will be need to be made.
Grahame
Briangoldcoast
1st May 2022, 04:03 PM
An excellent piece of kit, Graham
:)