View Full Version : Need Hercus parts anyone?? I wonder how this happened!!
Burner
23rd Mar 2015, 02:25 PM
Just saw this on Grays
http://www.graysonline.com/lot/0001-8001653/engineering-and-toolmaking/hercus-lathe-seaton-sa
WCD
23rd Mar 2015, 03:46 PM
That's sad. Fell on its face most likely.
I have seen it happen due to incompetent handling when moving a lathe.
Bill
Burner
23rd Mar 2015, 06:30 PM
How much of a fall would it take to crack the bed though?
WCD
24th Mar 2015, 07:55 PM
How much of a fall would it take to crack the bed though?
Who knows, but cast iron is brittle, and with a heavy headstock like that maybe just a fall off a pallet would do it.
Bill
Ueee
25th Mar 2015, 11:53 PM
Of all the Hercus's they could have dropped! If it was a model C i wouldn't give a stuff, but not a geared head like that (not sure on the model?)
Powered by vBulletin® Version 4.2.5 Copyright © 2024 vBulletin Solutions Inc. All rights reserved.