Corin
17th Jan 2014, 10:21 PM
I just bought a few more toys for my shop.
The first two are a Cone Mandrel and Swage Block. New, as cast. They need a little bit of dressing up but I have always wanted a giant steel witches hat!
http://i665.photobucket.com/albums/vv17/corinkayaker/cone_zps1d64c457.jpg
http://i665.photobucket.com/albums/vv17/corinkayaker/photo_zpsea05a1c1.jpg
The second is only on order at the moment... A 25 KG Anyang Power Hammer.... Wont see it for a few months but still pretty excited. Got a good price though the bulk buy being run by Anyang Australia...
http://youtu.be/FZP8Bhv8rcY
I just need to settle on what extra Dies to get. So many options...
Anyang Hammers Australia (http://www.anyangaustralia.com.au/dies.html)
The first two are a Cone Mandrel and Swage Block. New, as cast. They need a little bit of dressing up but I have always wanted a giant steel witches hat!
http://i665.photobucket.com/albums/vv17/corinkayaker/cone_zps1d64c457.jpg
http://i665.photobucket.com/albums/vv17/corinkayaker/photo_zpsea05a1c1.jpg
The second is only on order at the moment... A 25 KG Anyang Power Hammer.... Wont see it for a few months but still pretty excited. Got a good price though the bulk buy being run by Anyang Australia...
http://youtu.be/FZP8Bhv8rcY
I just need to settle on what extra Dies to get. So many options...
Anyang Hammers Australia (http://www.anyangaustralia.com.au/dies.html)