Hi everyone

Follwing my last post about homemade sand I thought you all maybe interested in my sand mixer as it saves a lot of work mixing the sand and breaking up the lumps after casting. Have a look at the video Foundry sand mixer - YouTube (http://youtu.be/r-fUMqtQ5L4)

.RC.
27th Jan 2013, 07:12 PM
Do you have any dimensions of the drum? Diameter, height etc...

giesser
28th Jan 2013, 11:44 AM
.RC.

The drum dia. is 600mm height is 150mm the rest can be adapted to what you can get hold of.

.RC.
28th Jan 2013, 01:04 PM
Thanks for the dimensions..