My draw bar is made from box section 65mm x 50mm x 3mm, I found out to late that you should not weld across the top of the drawbar at the point where it goes under the front cross beam, as it can eventually fracture at this point from fatigue. .
To overcome this problem I was thinking of stitch welding some Flat bar 250mm x 50mm x 6mm at this point on either side of the box section. Do you think this will help or does anyone have expierence or a proven solution that may help overcome this problem.
thanks in advance tigershark
To overcome this problem I was thinking of stitch welding some Flat bar 250mm x 50mm x 6mm at this point on either side of the box section. Do you think this will help or does anyone have expierence or a proven solution that may help overcome this problem.
thanks in advance tigershark