    Default Plumbers Solder Applications?

    Can basic plumbers solder normally used for copper pies etc be used on any other metals for simple repairs?, or is the next step up to use silver solder?

  2. #2
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    4,780

    Default

    It depends on the strength and fluid tightness requirements of your application.
    If it's a leak in a galvanised watering can it will be fine. If its something that has to bear a significant weight it won't.
    What are you intending to repair?

  3. #3
    Join Date
    Apr 2018
    Location
    USA
    Age
    53
    Posts
    14

    Default

    I'm repairing a vintage fan cage, thin steel wire, silver brazing rods seem expensive so I was trying to see if plumbers solder would work. I tried an experiment and it did not.

  4. #4
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    4,780

    Default

    Quote Originally Posted by Ken_Metal_Work View Post
    I'm repairing a vintage fan cage, thin steel wire, silver brazing rods seem expensive so I was trying to see if plumbers solder would work. I tried an experiment and it did not.
    What material is the fan cage made of, how are you cleaning it, are you using any flux, what sort of soldering iron are you using?
    What RPM is the fan?

    Again photos of the joints and describing what you are doing might help.

  5. #5
    Join Date
    Apr 2018
    Location
    USA
    Age
    53
    Posts
    14

    Default

    I was only asking if plumbers solder can be used to braze steel, on further research it seems it cannot so I'm not pursuing this line of thought any further - thanks

  6. #6
    Join Date
    Oct 2006
    Location
    Armidale NSW
    Age
    48
    Posts
    902

    Default

    Quote Originally Posted by Ken_Metal_Work View Post
    ... on further research it seems it cannot ...
    I've soldered steel to steel with both silver solder (15%) and soft solder.
    Cheers.

    Vernon.
    __________________________________________________
    Bite off more than you can chew and then chew like crazy.

  7. #7
    Join Date
    Apr 2018
    Location
    USA
    Age
    53
    Posts
    14

    Default

    I tried plumbers solder and it just fell off the steel, what type of flux is required?

  8. #8
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    4,780

    Default

    Quote Originally Posted by Ken_Metal_Work View Post
    I tried plumbers solder and it just fell off the steel, what type of flux is required?
    You need scrupulously cleaned pieces of steel - ie no oil, grease so a solvent clean first, then sanded with new paper, and a flux like Bakers flux. It works easier if you pre-tin (cover join area with a thin layer of solder) the steel surfaces independently and then heat and mate the surfaces and then run more soldier in . Surfaces should be a very neat fit if you want strength.

  9. #9
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    4,780

    Default

    Sorry if this sounds blunt but it really would save an awful lot of PPP "ping pong posts" and time if you tell us exactly what you did, materials and soldering iron you used and even photos of what you are trying to solder so that we can provide advice in a reduced number of replies.

  10. #10
    Join Date
    Apr 2018
    Location
    USA
    Age
    53
    Posts
    14

    Default

    Thanks for the replies, I'm closing this thread - not going to try and use plumbers solder for steel

Similar Threads

  1. Will solder hold?
    By Brickie in forum METALWORK GENERAL
    Replies: 29
    Last Post: 31st Dec 2007, 04:14 PM
  2. Welding applications and thin metal
    By Grahame Collins in forum WELDING
    Replies: 21
    Last Post: 10th Nov 2007, 01:36 AM
  3. Aluminum Solder
    By Nurgle in forum METALWORK GENERAL
    Replies: 7
    Last Post: 2nd Aug 2007, 12:46 PM
  4. Solder Flux?
    By Walesey in forum METALWORK GENERAL
    Replies: 5
    Last Post: 19th Jun 2007, 05:54 AM
  5. Silver Solder Pt 2 How to
    By Grahame Collins in forum METALWORK GENERAL
    Replies: 0
    Last Post: 11th Jan 2007, 10:51 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •