Results 1 to 12 of 12
  1. #1
    Join Date
    Dec 2018
    Location
    Perth, West Australia
    Age
    58
    Posts
    23

    Default Hercus power hacksaw

    Hi, I have access to a Hercus power hacksaw, good condition except the large casting at the top is shattered. Is it worth saving, and if so, anyone know of any parts source?
    Any info or views gratefully appreciated

  2. #2
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    54
    Posts
    5,042

    Default

    G'day Johnny
    Welcome to the forum. Without a picture or two so we can see what the damage looks like, that is a difficult call to make.You could either get it brazed up together or fabricate a new version from steel sections.
    Power hacksaws are a slow way of cutting things and while they still work (and a few people still use them) lots of members here have small horizontal bandsaws. These are faster, easier to find blades for and a bit more flexible as to what you can do with them. A basic version is probably a few hundred dollars (less if second hand) and are one of those bits of kit that seem to last forever. Depending on the damage, you could probably spend the cost of one of these fixing the hacksaw.

    Michael

  3. #3
    Join Date
    Dec 2007
    Location
    Sydney
    Posts
    83

    Default

    Depends on you aesthetic sensibilities.
    Spend the time and/or money and have a nice bit of old Aussie kit or go cheap Chinese.
    I was amused at a mate trouble shooting one of these but as Autobody restorers itís not an everyday item. It was only loose wires in the 3phase plug anyway.
    Heís also got on old Hercus lathe and chasing their mill for his home set up.
    Personally I use a Brobo plus an old Macpherson gearbox metal bandsaw
    Works for me although I know the set and forget feature of the other saws are useful.
    H.
    Jimcracks for the rich and/or wealthy. (aka GKB '88)

  4. #4
    Join Date
    Dec 2018
    Location
    Perth, West Australia
    Age
    58
    Posts
    23

    Default

    I dont need one, its just I hate to see good things wastedhercussaw.JPG

  5. #5
    Join Date
    Dec 2018
    Location
    Perth, West Australia
    Age
    58
    Posts
    23

    Default

    if anyone around Perth is interested let me know 0411080999

  6. #6
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    67
    Posts
    3,860

    Default

    Any chance of a pic of the damage, PLEASE?
    Kryn
    To grow old is mandatory, growing up is optional.

  7. #7
    Join Date
    Dec 2018
    Location
    Perth, West Australia
    Age
    58
    Posts
    23

    Default

    sm2.JPGThis is the only other pic I have, prior to the shattering of the casting. The offending item is under the cylindrical weight to the right of the pic. I will take some better ones next time im there

  8. #8
    Join Date
    Mar 2011
    Location
    Dural NSW
    Age
    77
    Posts
    1,156

    Default

    Hercus Hacksaw Machine
    These are a well built Australian Hercus machine.
    There was a new one of these in the Meadowbank NSW Tech college workshop when I was doing apprentice training there, in 1958.
    Seems a long time ago I was 17 yrs old & can remember the quality of the unit.
    Would be worth restoring !
    regards
    Bruce

  9. #9
    Join Date
    Aug 2012
    Location
    Greenmount, W.A.
    Age
    65
    Posts
    48

    Default

    Hello Johnny,
    I have sent you a PM.
    To find it, at the top of the page after you log on there is a tap "Notifications."
    Regards,
    Alan.

  10. #10
    Join Date
    Dec 2018
    Location
    Perth, West Australia
    Age
    58
    Posts
    23

    Default

    hercus.JPGThe offending damaged item

  11. #11
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    67
    Posts
    3,860

    Default

    Hi Johnny, that should be repairable. Grinding it to a V and then Brazing would facilitate a good repair. After, it could be sanded back then painted, probably wouldn't show the repair then either. If you managed to get it for free it would be a worthwhile project.
    Kryn
    To grow old is mandatory, growing up is optional.

  12. #12
    Join Date
    Aug 2015
    Location
    Melbourne, Australia
    Posts
    463

    Default

    If you've not already saved it or changed your mind, then .. that part is not really load bearing. Some cleaning and brazing may do it.

    I hate seeing old machinery die as well. You know, they only made 1700 of those things (according to here: https://australianmetalworkinghobbyi...ormation_id=14), so it's not like they're so thick on the ground you trip over them. If they only made that many I think every one of them is worth saving.

    I wish I'd saved my Mother's old EK Holden ... and they made a lot more of them .... but seen any on the road lately .... ? Nope. Save what you can. They are part of Australia's war history. They only made 1700 .....

Similar Threads

  1. Hercus Power Hacksaw
    By Petip in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 2
    Last Post: 22nd Apr 2017, 08:42 AM
  2. Hercus power hacksaw
    By snapatap in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 0
    Last Post: 26th Mar 2016, 08:54 PM
  3. Hercus power hacksaw attachment!
    By neksmerj in forum METALWORK GENERAL
    Replies: 2
    Last Post: 19th Dec 2012, 08:15 PM
  4. Hercus power hacksaw
    By Gavin Newman in forum METALWORK GENERAL
    Replies: 12
    Last Post: 14th Oct 2010, 08:51 PM
  5. Hercus 6a power hacksaw
    By footz in forum THE HERCUS AREA
    Replies: 7
    Last Post: 10th Oct 2008, 03:18 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •