    Thanks for all the replies, I'm going with the ATF on the mill as its an all metal pump and plumbing system.

    Next questions, what does ATF do to plastics.
    I see it's sold in HDPE containers so it has to be OK for that but what about other plastics.

    On the lathe I use a water feature pump. I think the body of the Pump is ABS.On the bandsaw the tank is PVC and the pump impeller and body could be nylon or PP.

  2. #17
    Join Date
    Apr 2009
    Location
    Ballina N.S.W.
    Posts
    587

    Default

    BobL,
    I fitted a fish tank pump on my band saw and it uses the same ATF as my other machines been running for years with no problems.
    Bob

  3. #18
    Join Date
    Jun 2007
    Location
    sydney ( st marys )
    Age
    59
    Posts
    4,022

    Default

    Do you run a central cooling system feeding all your machines?

  4. #19
    Join Date
    Apr 2009
    Location
    Ballina N.S.W.
    Posts
    587

    Default

    pipeclay,
    No each machine has its own system.
    Bob

  5. #20
    Join Date
    Jul 2013
    Location
    BRISBANE BAYSIDE
    Posts
    61

    Default

    krisfarm,
    How long does the ATF last? Does it have to be replaced at all? Is there any loss that needs to be topped up?
    Sorry about all the questions but I'm quite interested in using it. I set up a coolant system for my lathe a while back, but have never been quite game to start using it with any of the soluble oils.
    Alan

  6. #21
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    4,188

    Default

    Quote Originally Posted by OLCDOG View Post
    krisfarm,
    How long does the ATF last? Does it have to be replaced at all? Is there any loss that needs to be topped up?
    I haven't used it but I imagine there are quite a few factors that determine top-up/replacement
    - evaporation is low to non-existant so would not be a problems.
    - some will be lost to smoke production.
    - some oil will alway be flung off and not caught by drip trays etc so it will just depend how careful you are, what speeds you use, and what guards you have in place etc
    - some oil will be taken away on hands, work pieces and work tools.
    - I imagine if you use a lot of other oils eg way oils, these will eventually contaminate the ATF but complete replacement will be years away unless you are a pro shop.

    So top up will be required but as evaporation is not a significant factor I would imagine not much is needed.
    I'm keen to go with STF manly because I hate cleaning out the soluble oil tanks.

  7. #22
    Join Date
    Apr 2009
    Location
    Ballina N.S.W.
    Posts
    587

    Default

    Hi Alan,
    BobL has covered most of the answers to your questions, I find you also loose some from the swarf you create, I usually leave the swarf in the tray overnight to let it drain.
    Bob

Page 2 of 2 FirstFirst 12

Similar Threads

  1. Metal lube/coolant issues
    By BobL in forum SAFETY FORUM
    Replies: 13
    Last Post: 24th Nov 2016, 09:31 PM
  2. Possible Rolls Royce Coolant tank
    By BobL in forum METALWORK GENERAL
    Replies: 9
    Last Post: 8th Feb 2014, 12:12 AM
  3. Coolant/Oil proof paint?
    By John H in forum METALWORK GENERAL
    Replies: 6
    Last Post: 26th Sep 2009, 10:11 PM
  4. Sizing for one square steel section inside another
    By jeremy in forum METALWORK GENERAL
    Replies: 2
    Last Post: 7th Aug 2008, 09:50 PM
  5. adding a coolant tank
    By Oldhack in forum METALWORK GENERAL
    Replies: 21
    Last Post: 24th Jun 2007, 01:24 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •