    Default Resin Casting in Silicon moulds for pattern making

    I'm working on some patterns at the moment and for scales of economy it is much cheaper to cast 12 parts in an 12x18" Flask than to do individual items.

    How to get 12 identical patterns to fit on a runner. First issue all parts need to be split patterns.

    My idea is to make one split pattern and then resin cast the halves in a silicon mould to get the 12 patterns and mount them on a plate. The items are purely decorative so I don't have to worry about shrinkage scales.

    Anyone else thought of doing this and was it successful?
    …..Live a Quiet Life & Work with your Hands

  2. #2
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    29
    Posts
    399

    Default

    I share my factory with a sculptor who is constantly making resin bucks from sillicone moulds with 3d printed masters and it seems very effective and really captures the detail. If you want to come and look at hos technique in person you are welcome to.

  3. #3
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,398

    Default

    Ralph, That would be good if we can get a suitable time in the next week.


    Sent from my iPad using Tapatalk
    …..Live a Quiet Life & Work with your Hands

Similar Threads

  1. Making a fitting as a mock casting
    By Michael G in forum METALWORK PROJECTS
    Replies: 5
    Last Post: 16th Nov 2015, 06:44 PM
  2. Vacuum assisted casting in core-sand moulds.
    By MuellerNick in forum THE FOUNDRY
    Replies: 22
    Last Post: 30th Oct 2012, 03:09 PM
  3. Casting polyester resin balls
    By Ueee in forum METALWORK GENERAL
    Replies: 11
    Last Post: 25th Aug 2012, 09:01 PM
  4. Pattern for making a cone/frustum from sheet metal
    By blaisecendrars in forum METALWORK GENERAL
    Replies: 4
    Last Post: 5th May 2009, 11:47 PM
  5. Moulding parts From Resin Instead Of Casting Metal
    By echnidna in forum METALWORK GENERAL
    Replies: 2
    Last Post: 27th Jan 2008, 12:50 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •