    Hi Nedshead - they look fine to me. Even on thin material, the 2.5mm rods are often easier to use as they don't whip around as much as the thin 1.6mm ones - so if they're working for you I wouldn't worry about going out and buying a pack of thinner ones. I definitely favour 6012's compared to 6013's due to the slag issues that Grahame refers to. My only other comment is that when you are working on the actual job the go is to put your tacks on the corners, which has 2 advantages - 1 is you have and uninterrupted length to weld along the joint and 2 is that it gives a good bead on the corners on which to start and finish your welds - which allows you to weld a bit hotter than you might otherwise get away with.
    Cheers
    Mick

  2. #17
    Join Date
    Jan 2004
    Location
    Mackay Qld
    Posts
    4,058

    Default

    You are dead right Mick,

    The corner tacks as well as being excellent starts and stops add a bit of volume to the wall thickness.
    The net result is you are not likely to burn through as the extra material acts like a heat sink.
    As well edge to edge welds give a good visual effect.By the time Nedshead finishes his frame the stick beads will look like good Mig welds given the practice he will have had.

    Grahame

Page 2 of 2 FirstFirst 12

Similar Threads

  1. How thin steel can I weld with mig
    By Arron in forum WELDING
    Replies: 24
    Last Post: 19th Jul 2017, 05:37 PM
  2. What's it like to TIG SS 316 thin wall?
    By gazza2009au in forum WELDING
    Replies: 19
    Last Post: 21st Jun 2017, 05:18 PM
  3. welding thin material with stick inverter
    By Mathuranatha in forum WELDING
    Replies: 5
    Last Post: 18th Feb 2012, 03:36 PM
  4. problem TIG butt welding thin material
    By Brendon5374 in forum WELDING
    Replies: 17
    Last Post: 15th Sep 2011, 08:51 AM
  5. To cut thin steel?
    By Ricardito in forum METALWORK GENERAL
    Replies: 10
    Last Post: 21st Feb 2011, 11:22 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •