    Now that I am lonely during the day I am keeping busy to pass the time by cleaning out the van. Over the years i have accumulated lots of copper fittings which are shop soiled and as such probably no one else wants as it will warrant cleaning them to use in refrigeration systems....time is money!

    Are there any problems with melting down and casting copper. One thing i was thinking of was heads for a hammer...or even a drift.

    Have lots of pipe too and although its sealed others will look at it as an unknown and possibly risky. Can never be too clean for internal of refrigeration systems!!!

  2. #2
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    625

    Default

    You could melt them no problem you just need a furnace, or know some one who has one, or you could sell them for non refrigeration use such as water or air lines

  3. #3
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    3,322

    Default

    Quote Originally Posted by China View Post
    You could melt them no problem you just need a furnace, or know some one who has one, or you could sell them for non refrigeration use such as water or air lines
    on its way to being to being built...been like that for a year or so...but I am building one...just taking a little bit longer than what I thought...now that I am retired it might never get finished...but you never know eh?
    Seriously, I must get around to it

    1/2 inch and 3/4 I will keep for around the house.... as for all the other our piping above 1/2 goes in increments of 1/8th up to 7/8... ie next size is 5/8...then comes 3/4 and then comes 7/8, then we miss 1 inch and go to 1-1/8, then 1-3/8, then comes 1-5/8...why...cos they did... thus making all the other sizes outside of plumbing practices.

  4. #4
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    625

    Default

    I know what you mean now when I retired I was supposed to have time to do my own stuff, trouble is every one thinks I have nothing to do so I
    still don't have any free time ( I need to learn how to say "no")

Similar Threads

  1. Melting brass for lost wax casting
    By inlay chris in forum THE FOUNDRY
    Replies: 4
    Last Post: 17th Jun 2016, 09:06 PM
  2. Melting aluminium
    By Ch4iS in forum THE FOUNDRY
    Replies: 32
    Last Post: 15th Aug 2009, 12:17 AM
  3. Melting Metal In Microwave
    By echnidna in forum METALWORK GENERAL
    Replies: 0
    Last Post: 13th Jan 2009, 11:09 AM
  4. Melting metals in a domestic microwave
    By echnidna in forum METALWORK GENERAL
    Replies: 0
    Last Post: 13th Jan 2009, 10:04 AM
  5. Melting Lenses
    By Chris Parks in forum WELDING
    Replies: 8
    Last Post: 1st Sep 2007, 10:59 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •