Search:
Type: Posts; User: rustynail
Search: Search took 0.00 seconds.
-
2nd Jun 2015, 12:54 PM
Thread: .22 Bolt Action Issue
by rustynail- Replies
- 10
- Views
- 8,984
Might be time to pull the bolt apart and give it...
Might be time to pull the bolt apart and give it a good clean as well.
-
27th Nov 2012, 11:19 AM
- Replies
- 60
- Views
- 29,326
You may like to have a look at The Coin Carvery...
You may like to have a look at The Coin Carvery web site. The chaps name is Andy Jenkins. He frets out pennies with a hand fret saw, right down to the words and the date. They are a dead set work of...
-
17th Feb 2012, 12:31 PM
Thread: Items for Sale
by rustynail- Replies
- 19
- Views
- 14,920
Would best offer in a given time frame help?
Would best offer in a given time frame help?
-
26th Oct 2011, 12:09 PM
Thread: Trailer add ons share them here
by rustynail- Replies
- 69
- Views
- 43,159
Isn't this the same as a tilting boat trailer?
Isn't this the same as a tilting boat trailer?
-
19th Oct 2011, 01:41 PM
Thread: Suspension Upgrade
by rustynail- Replies
- 17
- Views
- 11,717
Depending on your method of attachment, your...
Depending on your method of attachment, your add-ons are going to compromise the galvanising on the existing trailer. As I understand it, these trailers are manufactured as a kit, to be shipped...
-
5th Oct 2011, 05:22 PM
Thread: DAM Rust....
by rustynail- Replies
- 24
- Views
- 15,776
Sorry to hear your story. Spent a fair bit of...
Sorry to hear your story. Spent a fair bit of time in Darwin straight after cyclone Tracy as a chippy. We had Tee shirts with "Shoota Loota" printed on them. Im sure you can relate to that. Just a...