Search:
Type: Posts; User: labr@
Search: Search took 0.00 seconds; generated 6 minute(s) ago.
-
12th Jul 2022, 10:06 PM
Thread: They are getting big
by labr@- Replies
- 21
- Views
- 10,390
Sounds amazing (and graceful) to me :U
Sounds amazing (and graceful) to me :U
-
19th Jun 2022, 03:35 PM
Thread: They are getting big
by labr@- Replies
- 21
- Views
- 10,390
Very impressive Vin. Looks like you need a PhD to...
Very impressive Vin. Looks like you need a PhD to operate it!
-
31st May 2022, 09:55 AM
Thread: Harden Cast iron Cylinders
by labr@- Replies
- 1
- Views
- 2,100
That would be a case hardening process such as...
That would be a case hardening process such as carburizing or nitriding. I have a very vague memory that nitriding is used on valve seats but could be wrong on that.
As for cast iron cylinders I... -
19th Apr 2022, 05:54 PM
Thread: foundry work or art
by labr@- Replies
- 5
- Views
- 4,227
So it's one of the bronzes - the colour had me...
So it's one of the bronzes - the colour had me wondering if it was pewter.
As for the last bell for the carillon, it may not be tuned yet but it sure sounds good on my tablet speaker. :2tsup: -
15th Apr 2022, 09:25 AM
Thread: foundry work or art
by labr@- Replies
- 5
- Views
- 4,227
Very nice Vin. At first I thought the clapper...
Very nice Vin. At first I thought the clapper would miss the bell, then realized that the sphere is the bit you hang on to. What metal did you use?
-
11th Feb 2022, 07:52 PM
Thread: They are getting big
by labr@- Replies
- 21
- Views
- 10,390
Looking good Vin. I have no experience with it...
Looking good Vin.
I have no experience with it but that looks like a large casting for the investment process.
Have you posted anything on the patterns and making the wax models? I'm interested in... -
I had to look up the meaning of carillon and am...
I had to look up the meaning of carillon and am surprised I hadn't come across it before.
How do you tune the bells? Is the tone mostly decided by size? -
Looks good Vin. Where do your bells end up? I can...
Looks good Vin. Where do your bells end up? I can picture them on river boats but the market there is probably somewhat limited these days.
-
19th Jan 2022, 11:46 AM
Thread: Casting pewter bell
by labr@- Replies
- 4
- Views
- 2,155
It's possible that the new source of pewter is...
It's possible that the new source of pewter is from Asia where they have a higher tin content at the expense of the antimony content - about 5% Sb in European pewter, about 1.5% in Asian.
If you... -
18th Aug 2020, 03:27 PM
- Replies
- 8
- Views
- 6,070
I don't know the formula to calculate the ideal...
I don't know the formula to calculate the ideal chill block size. However it looks like the cooling action needs to be fairly strong to be effective because most of the contraction in the boss needs...
-
18th Aug 2020, 12:55 PM
- Replies
- 8
- Views
- 6,070
Well it's easier to understand why you are...
Well it's easier to understand why you are thinking of using chill blocks now - there doesn't seem to be any easy way of applying risers to some of those areas.
At the risk of causing more... -
17th Aug 2020, 09:03 PM
- Replies
- 8
- Views
- 6,070
Chill blocks might help but they might make...
Chill blocks might help but they might make things worse. It's very dependant on the actual shapes involved. Posting some images of the pattern may help others with providing useful advice.
Have... -
20th Jan 2020, 10:55 AM
Thread: Lost Wax vs. Clay Casting
by labr@- Replies
- 2
- Views
- 7,255
Clay casting is similar to casting in sand moulds...
Clay casting is similar to casting in sand moulds in the sense that there is a parting line. This would probably not allow you to mould all the features that you need, such as the claws that hold the...
-
26th Oct 2019, 07:41 PM
Thread: Cast iron question
by labr@- Replies
- 6
- Views
- 7,299
For the original question I'd go with what Greg...
For the original question I'd go with what Greg said.
With regard to annealing, the casting will still be brittle compared to steel - grey cast iron is an inherently brittle material due to the... -
17th Jun 2016, 09:06 PM
Thread: Melting brass for lost wax casting
by labr@- Replies
- 4
- Views
- 5,124
Why can't you melt the metal in another...
Why can't you melt the metal in another furnace/crucible and then pour it into the crucible on the machine?
Can you post a pic of the machine? It may help to illustrate the limitations /... -
6th Feb 2016, 01:17 PM
Thread: A Question About Pouring Cast Iron
by labr@- Replies
- 5
- Views
- 5,383
A late reply I know but I've only just stumbled...
A late reply I know but I've only just stumbled on to this forum.
Texx is right, it would be ferrosilicon or a proprietary inoculant based on ferrosilicon.
The late addition of a small quantity...