Search:

Type: Posts; User: Chas

Page 1 of 3 1 2 3

Search: Search took 0.01 seconds.

  1. Replies
    12
    Views
    1,445

    You can ensure the oil you buy is non-corrosive...

    You can ensure the oil you buy is non-corrosive to copper based alloys if it is specified GL-4. Avoid GL-5 oils.

    Chas.
  2. Thread: Cast repair

    by Chas
    Replies
    21
    Views
    4,271

    Hello Greg, Thanks for updating my knowledge, my...

    Hello Greg,
    Thanks for updating my knowledge, my welding experience is limited to OA and Stick. Tig is not something I have ever used.

    Chas.
  3. Thread: Cast repair

    by Chas
    Replies
    21
    Views
    4,271

    I am somewhat surprised at the several...

    I am somewhat surprised at the several recommendations for silicon bronze in this scenario. When I did the 2Yr Advanced Oxy Acetylene Welding course at a NSW Technical College (now TAFE), the...
  4. Replies
    6
    Views
    1,852

    Amen to to the opinion and advice offered by...

    Amen to to the opinion and advice offered by China. Try to ensure the brazing is carried out using manganese bronze filler rod. Perhaps Grahame Collins might care to offer further suggestions....
  5. I would use an oxy/acetylene cutter to remove the...

    I would use an oxy/acetylene cutter to remove the core slug. A #15 tip would cut that thickness material; you would need to drill a single hole on the pitch circle of the cutout, then begin the...
  6. Thread: Scary welder

    by Chas
    Replies
    10
    Views
    1,424

    It's hard to tell from the picture, but it looks...

    It's hard to tell from the picture, but it looks like an old "Samson" brand welder. I had one offered to me for sale S/H in the 1960s, but bought an EMF Transarc 200 instead from the seller. The...
  7. Replies
    19
    Views
    2,892

    The chips from the machining look different from...

    The chips from the machining look different from my experience with grey cast iron. I suspect the cranks are cast from spheroidal graphite (SG) cast iron which is a legitimate and common material...
  8. Replies
    26
    Views
    6,098

    It might be possible to cut the stud out of the...

    It might be possible to cut the stud out of the centre of the nut by using an end-mill of the same size as the stud and held in an electric drill. As the stud is heat treated, this will not be easy....
  9. Replies
    26
    Views
    6,098

    I totally agree, except that a slightly blunt...

    I totally agree, except that a slightly blunt chisel will be better if you are trying to undo the nut rather than split it. Another way, provided that you can remove the brake caliper with the wheel...
  10. Replies
    154
    Views
    43,858

    4" mini electric chainsaw from China, beware!

    I recently ordered an unbranded 4" 550w 24V handheld mini chainsaw from an ebay seller which was Chinese but listed as "Australian stock". The item arrived after about a week, and required assembly...
  11. Replies
    154
    Views
    43,858

    Thanks QC, Typo duly noted and corrected. Chas.

    Thanks QC, Typo duly noted and corrected.

    Chas.
  12. Replies
    154
    Views
    43,858

    I ordered a replacement Husqvarna chainsaw...

    I ordered a replacement Husqvarna chainsaw clutch cover for my S.I.L on 27/01/2021 and it arrived on Thursday 11/03/2021. It is slightly different from the ebay picture, but I think it is the...
  13. Replies
    9
    Views
    6,330

    Feel free, I am glad you have found the photo...

    Feel free, I am glad you have found the photo useful. I think the colour was slightly brighter when new, but now looks darker due to imbedded grime.

    Chas
  14. Replies
    9
    Views
    6,330

    As requested. Chas. 390039

    As requested.

    Chas.


    390039
  15. Replies
    9
    Views
    6,330

    My 5'' offset CI Joplin came new in the late...

    My 5'' offset CI Joplin came new in the late 1950's painted orange. That was the normal colour for that period.

    Chas.
  16. Replies
    7
    Views
    2,896

    From the picture of the charger, the word...

    From the picture of the charger, the word "AUTOMATIC" across the front might be a clue. Most automatic chargers will only output a charging current if connected to a battery which has a voltage...
  17. I am having a problem with (2) for the simple...

    I am having a problem with (2) for the simple reason that acetylene cylinders are by law manufactured with one or more fusible plugs which are designed to ensure that the scenario you describe does...
  18. Replies
    23
    Views
    6,901

    Some specialty steel supplies like Bohler...

    Some specialty steel supplies like Bohler Uddeholm who have a large set of shelves with a reasonable collection of speciality short pieces for sale.[/QUOTE]

    Bob, if you have access to BU at the...
  19. Replies
    9
    Views
    2,120

    Well, my Moore & Wright #961 does not have...

    Well, my Moore & Wright #961 does not have carbide anvils, but I wouldn't call it "cheap or nasty". It has served me well over a lifetime, as has an M&W 0-4" adjustable mic, also without carbide...
  20. Replies
    15
    Views
    6,734

    In the US the older standard colours for AC line...

    In the US the older standard colours for AC line cords was black active, white neutral, and green earth. As far as I recall, DC has always been red+ and black-.

    Chas.
  21. Replies
    10
    Views
    4,037

    You will find that chainsaw bar oil which...

    You will find that chainsaw bar oil which contains a tackifier will be more than suitable as a way oil. It is available in one litre quantities for around $10.

    Chas.
  22. Replies
    6
    Views
    4,613

    15A Plug to 10A Socket (Again)

    Hello All,
    This weeks Aldi catalogue (P16) has a solution for those who see a need to connect 15A rated tools and devices to a 10A socket. As this "15A-10A Safety Adapter" is for sale as a...
  23. Thread: 17 tpi thread

    by Chas
    Replies
    24
    Views
    10,462

    Pipeclay is correct, a 24/51 gear combination...

    Pipeclay is correct, a 24/51 gear combination will give you 17 TPI. As far a I can determine, Hercus did not have a 51 tooth gear in their parts list, so you will need to find a custom made one if...
  24. Replies
    9
    Views
    2,912

    I have one of approximately that vintage, and the...

    I have one of approximately that vintage, and the spindle threads are 5/8"-18 TPI NF thread.

    Chas
  25. Replies
    16
    Views
    4,378

    Aldi had a product on their periodic specials...

    Aldi had a product on their periodic specials which might be suitable. It is called Deco Style Transparent Protection Spray, in a 384g rattle can. It promises "perfect protection for metal, wood and...
  26. Replies
    33
    Views
    5,942

    Then i won tattslotto... the wind changed, lucky...

    Then i won tattslotto... the wind changed, lucky for me but not for the poor buggers that lived in chum creek.
    As the fire took off up that valley the relative silence was punctuated by exploding LP...
  27. It turned out that someone had turned off the...

    It turned out that someone had turned off the steam supply to the tank and the chocolate had set stopping the mixer blades and in turn the motor and causing it to burn out.

    There were three of...
  28. Replies
    18
    Views
    4,729

    I suggest you avoid placing the lathe in line...

    I suggest you avoid placing the lathe in line with the N/S terrestial magnetic lines of force at your location if possible. The result will otherwise be that everything ferrous that you turn will...
  29. Replies
    4
    Views
    4,867

    Can't help about the ties, but there is a...

    Can't help about the ties, but there is a possibility the router is powered by 400HZ which was popular in the WW2 period. The motor certainly looks like an induction motor.

    Chas.
  30. Replies
    26
    Views
    12,870

    [QUOTE=Hunch;1948097]Is the black soot really...

    [QUOTE=Hunch;1948097]Is the black soot really avoidable? Still have to put up with it at the beginning in any event. /QUOTE]

    To avoid this, contained in the Linde Air Products book 'The...
  31. Caskwarrior, It might be worth a call to Mick...

    Caskwarrior, It might be worth a call to Mick Moyle's in Sydney. They have all kind of stuff, both new & SH.

    Chas.
  32. Replies
    102
    Views
    24,723

    Could you please provide a reference for this...

    Could you please provide a reference for this oft-quoted statement? My copy of AS/NZ 3018-2001 'Electrical Installations - Domestic Installations' has on p62 a Table 6-1 "Guidance on the number of...
  33. Replies
    26
    Views
    8,945

    I would just cut a suitable groove (6mm?) across...

    I would just cut a suitable groove (6mm?) across the face of the protector and use a piece of the same sized bar in the groove to unscrew the protector. Not pretty, but simple and guaranteed to...
  34. Thread: Gloves at work

    by Chas
    Replies
    56
    Views
    14,973

    In my early life involving Technical College (now...

    In my early life involving Technical College (now TAFE) and metal working trades, the combination of gloves and grinders was strictly forbidden. It is so easy for a glove to catch between a tool...
  35. Replies
    19
    Views
    12,972

    Thanks for the information, Bob. It is always...

    Thanks for the information, Bob. It is always good to learn something new. My remarks were in the context of a woodworking bandsaw, due in part to what appears to be a layer of sawdust on the motor...
  36. Replies
    19
    Views
    12,972

    I'm not sure why you have so much enthusiasm for...

    I'm not sure why you have so much enthusiasm for a VFD on a bandsaw. Surely, unlike a lathe, mill or drill, there is no compensation required for the size of the work or cutter. I would suggest...
  37. Replies
    8
    Views
    3,799

    You will need an extra 140mm minimum clearance...

    You will need an extra 140mm minimum clearance between a wall and the headstock cover in order to be able to open it.

    Chas.
  38. Thread: No mess cast iron

    by Chas
    Replies
    4
    Views
    1,335

    I concur. Chas.

    I concur.

    Chas.
  39. Thread: Burst Capacitor

    by Chas
    Replies
    4
    Views
    3,149

    The ruptured capacitor network is an EMI filter...

    The ruptured capacitor network is an EMI filter to limit electrical noise being fed back into the mains. The operation of the motor is not dependent on it, the manufacturer has probably included it...
  40. Replies
    7
    Views
    3,857

    Bob, I would be surprised if the motor shown is...

    Bob, I would be surprised if the motor shown is more than 1HP. I think your assumption of 20% losses for inefficiencies is being rather conservative, given the class of motor and the fact that it is...
  41. Replies
    22
    Views
    10,973

    Hello Joe, You will find it easier to perform a...

    Hello Joe,
    You will find it easier to perform a downhand fusion weld on CI if you are able to incline the work at about 30 degrees up from horizontal. This keeps the top of the weld pool...
  42. Replies
    15
    Views
    4,943

    Hello BaronJ, I think your interpretation of...

    Hello BaronJ,

    I think your interpretation of what you describe as a folding crank handle on the magneto in pic#3 may be incorrect. That looks like the normal end cover retainer which consists of...
  43. Thread: oil

    by Chas
    Replies
    5
    Views
    2,960

    Wouldn't that be ISO 68, which is roughly...

    Wouldn't that be ISO 68, which is roughly equivalent to SAE 20? I am not aware of any SAE grade 68.

    Chas..
  44. Replies
    12
    Views
    5,822

    Up to the 1960's, red was the designated colour...

    Up to the 1960's, red was the designated colour for AC earth wiring in Germany. Perhaps the wire on that VFD had its origins in that country, or someone from there?

    Chas.
  45. Replies
    12
    Views
    5,822

    [QUOTE=StrayAlien;1933465]Chas, thanks. No delta...

    [QUOTE=StrayAlien;1933465]Chas, thanks. No delta in there? Is that what you mean?

    Yes, no delta option; the motor is wired either 440V star (HI Voltage) or 220V star (Lo Voltage). I would think...
  46. Replies
    12
    Views
    5,822

    According to my understanding of the motor...

    According to my understanding of the motor connection diagrams on the nameplate, the motor is star connected for either 440V or 220V. The windings to (7), (8), and (9) are internally connected...
  47. Replies
    15
    Views
    9,843

    Two weeks???; I wish. I am still waiting for an...

    Two weeks???; I wish. I am still waiting for an item shipped from China which according to tracking, arrived in Melbourne on 4th December. Unfortunately, Australia is one of the very few countries...
  48. Replies
    7
    Views
    13,045

    According to the Richardson sales brochure,...

    According to the Richardson sales brochure, speeds for a standard machine are 350, 650, 1100, 2000, 3500, and 5500 rpm. Sterling and Richardson machines are identical, this was a badge-engineered...
  49. Hello Ross, I have to ask, why are you so...

    Hello Ross,

    I have to ask, why are you so eager to replace the oil in the welder? Shell Diala B Transformer Oil was an industry standard for decades, and the fact that it is "obsolete" probably...
  50. Replies
    7
    Views
    3,249

    The "Trash & Treasure" market at Prestons has...

    The "Trash & Treasure" market at Prestons has recently closed to become a housing development. Many of the sellers have moved to the Sunday Market at the Blacktown Drive-In Cinema site near the...