Yep, just the one bowl that comes on the cutter....
Yep, just the one bowl that comes on the cutter. Don't have that problem in the shed where the compressor setup has a decent condensation management system :D
In the shed on clean steel 5-6m is... -
4th Mar 2013, 08:37 PM
- Replies
- 3
- Views
- 8,513
Long Term Review of Token Tools LG-40E Plasma Cutter.
Hi Forum,
18 months ago I bought a Token Tools LG40E plasma cutter for home use. I also have a 200A ac/dc tig of the same brand. I have no other connection to Peter other than being a happy... -
13th Jan 2013, 11:36 AM
- Replies
- 4
- Views
- 7,792
N.S.W. This item has been sold.
This item has been sold.
-
12th Jan 2013, 08:22 PM
- Replies
- 4
- Views
- 7,792
N.S.W. Hi Anton, I bought it at a auction of gear...
Hi Anton,
I bought it at a auction of gear from a high school metalwork dept. The bare metal surfaces had a surface coating of rust and I wire wheeled it off. Going off the serial number I... -
8th Jan 2013, 05:52 PM
- Replies
- 4
- Views
- 7,792
N.S.W. Magnabend 1000E Sheetmetal Folder LOC: Coffs Harbour NSW
For sale is my Magnabend 1000E Sheetmetal Folder. Bending capacity is 1000x1.6mm.
Uses an electromagnetic clampbar to hold the material which means you can achieve shapes not normally capable of... -
8th Jan 2013, 05:42 PM
- Replies
- 0
- Views
- 6,934
N.S.W. Hafco AL330 Metal Lathe LOC: Coffs Harbour NSW
Decided to sell my lathe. I just don't use it enough to justify it sitting in the garage, especially when I have access to all the gear I could possibly need at work.
Is about 10 years old, has a... -
20th Sep 2012, 09:22 PM
Thread: Cast iron welding questions
by BenM78- Replies
- 15
- Views
- 11,227
I've done a few cast iron repairs at work. ...
I've done a few cast iron repairs at work.
Get the nickel rods and turn your amps down 70-80 for 3.2 rods.
Do short runs just to build up the weld. In between runs peen the weld area with... -
20th Sep 2012, 09:11 PM
Thread: Building up teeth on a gear cog
by BenM78- Replies
- 1
- Views
- 5,581
If it is cast iron you should be able to weld it...
If it is cast iron you should be able to weld it up. You'll need some nickel rods made for welding cast iron. I'd weld one tooth up at a time and clean up with a grinder as you go to give a reference...
-
3rd May 2012, 10:53 PM
Thread: Gas Vs Gasless
by BenM78- Replies
- 31
- Views
- 20,950
How intriguing. Would cost bugger all to put a...
How intriguing. Would cost bugger all to put a rectifier in there and have something that might actually work!
I love these kinds of machines, people buy them, can't do anything with them and then... -
3rd May 2012, 08:07 AM
Thread: Gas Vs Gasless
by BenM78- Replies
- 31
- Views
- 20,950
I'd doubt that your welder is AC on the output....
I'd doubt that your welder is AC on the output. Mig is a DC process. Stick is the best choice for gasless welding on a home type level.
-
28th Apr 2012, 09:37 PM
Thread: Anti-spatter spray
by BenM78- Replies
- 8
- Views
- 8,036
We use a water based soapy pink product at work,...
We use a water based soapy pink product at work, can't think of what the name is off hand. I personally don't use it as I'm with Karl - spatter is controllable by doing it right! Too much gun angle...
-
25th Apr 2012, 08:49 AM
Thread: Having trouble welding a T joint
by BenM78- Replies
- 16
- Views
- 15,710
I have a box of chinese electrodes that are hard...
I have a box of chinese electrodes that are hard to control as the OP described. At work we use the WIA Austarc 12's and 13's and they are a joy. Don't be afraid to turn it up either.
Was talking... -
24th Apr 2012, 10:51 PM
Thread: Tungsten Sharpening Tip
by BenM78- Replies
- 1
- Views
- 5,214
Tungsten Sharpening Tip
Just thought I'd share a tip with you all.
When sharpening your tungsten for tig welding on a bench grinder, put the tungsten in your battery drill and pull the trigger whilst applying tip to the... -
29th Nov 2011, 10:02 PM
Thread: reg not facing the right way up?????
by BenM78- Replies
- 14
- Views
- 8,883
What Tokentools will give you that random ebay...
What Tokentools will give you that random ebay cheapies won't...
5 year warranty
A phone number that you CAN ring and WILL be answered
I have both a tig and a plasma of Petes and don't know... -
29th Nov 2011, 06:15 AM
Thread: gloves for metalworking?
by BenM78- Replies
- 106
- Views
- 53,642
Pretty much, if I grabbed my drill chuck with two...
Pretty much, if I grabbed my drill chuck with two gloved hands I'd be able to stop it, especially being belt driven. Geared head lathes have no slip and will eat people whole.
-
28th Nov 2011, 09:55 PM
Thread: gloves for metalworking?
by BenM78- Replies
- 106
- Views
- 53,642
Dean, many years ago on my way home from work I...
Dean, many years ago on my way home from work I came across an abandoned EF falcon sedan. The bonnet was heavily caved in and a dead roo on the roadside 30m or so back. The airbag had deployed.
... -
22nd Nov 2011, 07:43 PM
Thread: Casting small engine parts
by BenM78- Replies
- 31
- Views
- 19,023
We get small run castings done at work, not cheap...
We get small run castings done at work, not cheap but I'll find out who does them if you like?
-
15th Nov 2011, 03:33 PM
Thread: The Ducks Guts For Cleaning Welding Visors
by BenM78- Replies
- 9
- Views
- 8,374
Same helmet, but I have no idea what the...
Same helmet, but I have no idea what the replacement screens cost, welding for the boss means the boss buys me new screens :P
Miller Elites don't carry an AS sticker anyway so polishing with... -
6th Sep 2011, 08:46 PM
Thread: Stainless TIG gas consumption
by BenM78- Replies
- 27
- Views
- 18,622
Had a look at the ones at work, all it says is...
Had a look at the ones at work, all it says is 'Made in USA' and safety/usage info.... no makers name nothing! I am fairly certain they came from Aitkens though so maybe just try a welding place and...
-
6th Sep 2011, 07:19 AM
Thread: Stainless TIG gas consumption
by BenM78- Replies
- 27
- Views
- 18,622
I'll find out today what brand they are and where...
I'll find out today what brand they are and where they come from. Normally though just any industrial supply house would have them.
-
5th Sep 2011, 08:44 PM
Thread: Stainless TIG gas consumption
by BenM78- Replies
- 27
- Views
- 18,622
Good stuff. To clean up your welds get hold...
Good stuff.
To clean up your welds get hold of a stainless blending disc. They are a creamy white colour and are cellulose based. Give a very fine grind unlike a flap disc or grind wheel. Have an... -
27th Aug 2011, 09:30 PM
Thread: Stainless TIG gas consumption
by BenM78- Replies
- 27
- Views
- 18,622
OK, looking at those pics I am sure the gas is...
OK, looking at those pics I am sure the gas is argon, if you use a argon/co2 blend on tig the outcome is very crusty on the surface.
2.4 electrode is fine, as is your grinding wheel. so long as... -
27th Aug 2011, 09:21 PM
Thread: Stainless TIG gas consumption
by BenM78- Replies
- 27
- Views
- 18,622
If I was welding this at work I'd be looking...
If I was welding this at work I'd be looking around 60 amps, 1.6 filler and 8lpm on a #6 nozzle.
This is about the best you can hope for straight off the torch, mostly welds will have a lot of... -
23rd Aug 2011, 09:28 PM
Thread: How do I TIG Weld 1mm Aluminium
by BenM78- Replies
- 23
- Views
- 24,404
After a lot of thought I finally had a go at this...
After a lot of thought I finally had a go at this today. I always thought that if MIG worked as a DC process to weld aluminium then there had to be a way of getting it to work on tig - then of course...
-
12th Aug 2011, 08:29 AM
Thread: Just got my Lincoln 180c -Not Good!!
by BenM78- Replies
- 18
- Views
- 19,499
This law has been the case for many many years. ...
This law has been the case for many many years.
When it comes to ebay, the only time it DOESN'T apply is for auctions, if you click 'Buy It Now' then it is a retail transaction and the Trade... -
12th Aug 2011, 08:20 AM
Thread: Pipe Bending Fail
by BenM78- Replies
- 33
- Views
- 25,207
Interference fit? What is the accepted method of...
Interference fit? What is the accepted method of removing the die after bending? Big Hammer?
-
11th Aug 2011, 08:35 PM
Thread: Pipe Bending Fail
by BenM78- Replies
- 33
- Views
- 25,207
You got it, but then I figured that would be the...
You got it, but then I figured that would be the case - I could have sought a refund through the Fair Trading 'Not Fit for Purpose' clause but the only alternative is an order of 10x more expensive...
-
16th Jul 2011, 04:26 PM
Thread: Pipe Bender WIN!
by BenM78- Replies
- 3
- Views
- 7,094
Pipe Bender WIN!
Further to this thread here - http://www.woodworkforums.com/f65/pipe-bending-fail-120570/
I came across a post on another forum that showed the results of heating the die, hammering it a... -
15th Jul 2011, 02:37 PM
Thread: Pretty welds
by BenM78- Replies
- 32
- Views
- 22,080
Just went and had a look back through some of my...
Just went and had a look back through some of my work pics, found one I liked, I think I am too hard on myself sometimes....
Pretty easy to achieve with a pulse tig and positioner though. 38mm... -
14th Jul 2011, 10:19 PM
Thread: Pretty welds
by BenM78- Replies
- 32
- Views
- 22,080
A lot of the welds, especially the 'weave' tig...
A lot of the welds, especially the 'weave' tig were heavily undercut and underfilled, It was explained somewhere that this is to increase the radius of the weld...
The mig welds had me cringing,... -
1st Mar 2011, 06:33 AM
Thread: welding extruded aluminium tube
by BenM78- Replies
- 8
- Views
- 8,422
Capral uses 6060T5 in their extrusions, some...
Capral uses 6060T5 in their extrusions, some qubelok is 15um clear anodised, some is mill finish.
-
1st Mar 2011, 06:26 AM
Thread: welding extruded aluminium tube
by BenM78- Replies
- 8
- Views
- 8,422
If you were using qubelok system then it is...
If you were using qubelok system then it is highly likely it was anodised. Grind a bit back with a blue flap disc and see how it goes.
-
28th Feb 2011, 08:04 PM
Thread: Need a good pair of snippers
by BenM78- Replies
- 14
- Views
- 6,516
lol, what a great thread :) Personally, I'd...
lol, what a great thread :)
Personally, I'd cut 0.9 316 all day with a pair of wiss snips, up to 40mm long. I sharpen my wiss set maybe twice a year and cut a lot of 0.9 to 1.5 316 in between. But... -
23rd Feb 2011, 05:24 AM
Thread: TIG welding helmets
by BenM78- Replies
- 91
- Views
- 54,853
I paid $70 more for my Miller Digital Elite...
I paid $70 more for my Miller Digital Elite helmet and was worth it, as I sent it back for a warranty claim as the LCD started to delaminate. One of the work provided helmets went back for warranty...
-
26th Jan 2011, 09:15 AM
Thread: Bitten the bullet
by BenM78- Replies
- 18
- Views
- 21,745
Just an update on how the machine is going... ...
Just an update on how the machine is going...
The gas solenoid is continuously not closing at the end of a weld, seems to be sticking open slightly. I have had the solenoid out and open to clean... -
3rd Jan 2011, 06:18 PM
- Replies
- 5
- Views
- 9,768
Thanks Ern, have posted the same Q to Myswag (was...
Thanks Ern, have posted the same Q to Myswag (was already a member there). Some quality builds go on over there!
-
3rd Jan 2011, 05:00 PM
- Replies
- 5
- Views
- 9,768
Hi, Nah not really the big aussie treks, just...
Hi, Nah not really the big aussie treks, just Barrington Tops, Upper Macleay valley, something that needs a bit of ground clearance and suspension to get into, 800km of corrugations is not my wifes...
-
3rd Jan 2011, 04:29 PM
- Replies
- 5
- Views
- 9,768
Caravan Modding - Specifically Viscount Aerolite
Been thinking of buying an old van to make camping that little bit more comfortable, however having a lifted GU Patrol on 33 muds means I like the offroad thing too... So I need something that is...
-
14th Dec 2010, 08:20 PM
Thread: Correct placement of split/spring washers
by BenM78- Replies
- 16
- Views
- 14,168
Correct placement of split/spring washers
Hi all, I am trying to find a definitive answer to a question that has been bugging me and a tradesman at work (difference of opinion...)
When using a split spring washer I was told (apart from... -
26th Oct 2010, 08:53 PM
Thread: Cheap 3" or 4" 3 Jaw Chuck
by BenM78- Replies
- 0
- Views
- 4,019
Cheap 3" or 4" 3 Jaw Chuck
Chasing a used cheap 3 jaw in the small size for a little project I have on, doesn't have to be the most accurate (ie within .2-.3mm tir would be fine) any kind of mount type is fine :)
Happy to... -
21st Oct 2010, 07:59 PM
Thread: Aluminium welding techniques
by BenM78- Replies
- 9
- Views
- 9,012
Ok, Started with 2 100x300x5mm plates today,...
Ok, Started with 2 100x300x5mm plates today, sanded all the surface of both plates with zirc flap disc.
Did a few welds, ended up finding 230 amps was the sweet spot (fronius pulse mig) 0 on arc... -
14th Oct 2010, 08:36 PM
Thread: Aluminium welding techniques
by BenM78- Replies
- 9
- Views
- 9,012
Thanks for that. I was supposed to be at tech...
Thanks for that. I was supposed to be at tech today to get back into it but had to look after sick kids - hopefully next week!
Yes it is extruded bar, I can get hold of some plate to try too... -
14th Oct 2010, 08:30 PM
Thread: Welding Carbide to SS
by BenM78- Replies
- 16
- Views
- 10,669
http://www.woodworkforums.com/f65/silver-solder-pt...
http://www.woodworkforums.com/f65/silver-solder-pt-1-info-43407/
We use the SB 45 at work for silver soldering stainless steel bit of an art to it , well not really. If the stainless gets too hot... -
11th Oct 2010, 08:22 PM
Thread: Where to get metal stock?
by BenM78- Replies
- 23
- Views
- 12,999
Can I assume the brass you are after is 1"...
Can I assume the brass you are after is 1" diameter and 2' in length? If you actually mean 1' and 2' then at $80, Pipeclay, I'll take ten!
But seriously there is a ton of engineering firms that'll... -
24th Sep 2010, 06:12 PM
- Replies
- 5
- Views
- 4,515
Midway do no 8 and have a store in Melbourne. We...
Midway do no 8 and have a store in Melbourne. We use them at work for most of our stainless. Either them or Atlas
-
24th Sep 2010, 08:29 AM
Thread: Aluminium welding techniques
by BenM78- Replies
- 9
- Views
- 9,012
sorry, it wasn't the whole weld that didn't stick...
sorry, it wasn't the whole weld that didn't stick only the start 10-15mm or so. Was using a fronius mig with torch control. Best results came with a starting amps of 205 then backing of one click...
-
23rd Sep 2010, 10:25 PM
Thread: 4' or 5' angle grinder
by BenM78- Replies
- 65
- Views
- 39,117
I bought my bosch as we have one on the tool wall...
I bought my bosch as we have one on the tool wall at work. I nearly always pick up the bosch over the metabo or hitachi grinders there. It is so light and the body is small despite the decent power....
-
23rd Sep 2010, 10:21 PM
Thread: Aluminium welding techniques
by BenM78- Replies
- 9
- Views
- 9,012
I started ally mig at tech today and that was the...
I started ally mig at tech today and that was the method taught to us.
My problem is getting the weld to stick at the start, broke a few welds that the bead just fell off. -
17th Sep 2010, 08:50 AM
Thread: 4' or 5' angle grinder
by BenM78- Replies
- 65
- Views
- 39,117
not really, depending on what I am doing I will...
not really, depending on what I am doing I will deliberately choose a worn disc rather than a new disc as it will give a smoother finish, like going to a finer grit. I am really interested in this...
-
15th Sep 2010, 07:46 AM
Thread: 4' or 5' angle grinder
by BenM78- Replies
- 65
- Views
- 39,117
5" Cutting, 4" Grinding I have a 5" Makita and...
5" Cutting, 4" Grinding
I have a 5" Makita and a 4" Bosch. The $85 blue Bosch kits are great, can't kill em, plenty of power.