    Restoration of a car ferry

    Hi,

    OK, it's not quite cars, but nearly. The Raymond Island car ferry, on the Gippsland Lakes, Vic., has been taken out of service after corrosion on its undersides was found.

    Apparently when...
  2. Replies
    8
    Views
    2,214

    I agree with Peter, I used to use shell end mill...

    I agree with Peter, I used to use shell end mill cutters with drive slots on the back like this

    https://3.imimg.com/data3/JK/QA/MY-7189258/shell-end-mills-250x250.jpg

    I note the square tongues...
  3. Replies
    6
    Views
    5,888

    Hi, With our ER11 collets I have notice the...

    Hi,

    With our ER11 collets I have notice the same puzzle, so am also interested.

    At the moment I order these router bits off eBay, usually from China, in HSS and carbide, 3 mm, 4 mm, 6 mm, and...
  4. Replies
    5
    Views
    4,969

    Hi, This is correct. The idea is the machine...

    Hi,

    This is correct. The idea is the machine operator (usually a thread rolling machine) can use it quickly to determine if thread size is correct, without having to make an actual measurement....
  5. Replies
    5
    Views
    1,732

    They are only for finishing a cut in tight spots...

    They are only for finishing a cut in tight spots I think. Routinely I use a simple nibbler attachment to a power drill and it works very well.

    Cheers
  6. Hi, We have a single phase lathe on which the...

    Hi,

    We have a single phase lathe on which the reversing switch fell to bits internally. We contacted an industrial electricians' company who were useless. The sparky knew nothing about it when he...
  7. Replies
    3
    Views
    2,205

    A used one you mean? Anywhat, here's one in...

    A used one you mean?

    Anywhat, here's one in eBay. I bought a single phase motor off this bunch, and it seemed quite good (I have no connection with them, to make a pun).

    3kw 4HP 1400rpm shaft...
  8. Thread: Vgroove

    by GeoffW1
    Replies
    8
    Views
    2,173

    Hi, I agree with Michael. The trouble with V...

    Hi,

    I agree with Michael. The trouble with V cutters in a vertical spindle machine is that the area near the tip of the V is at very much non-ideal cutting conditions, with very slow surface...
  9. Thread: Router bits

    by GeoffW1
    Replies
    11
    Views
    4,121

    Hi, I think they would be a better choice than...

    Hi,

    I think they would be a better choice than HSS router bits, due to the cutting edge angle being relatively more suitable for aluminium than the fairly acute edge on the HSS bits. Then of...
  10. Replies
    4
    Views
    1,858

    Recall on Swarts 14" cutoff saw, Jan 2017

    Swarts Tools — 14" Metal Cut Off Saw | Product Safety Australia
  11. Thread: Grinding Wheel

    by GeoffW1
    Replies
    18
    Views
    3,713

    Hi, Blackwoods lists the type 6 straight cup...

    Hi,

    Blackwoods lists the type 6 straight cup wheel in general purpose grades

    https://www.blackwoods.com.au/search/grinding-wheels-straight-cup-type-6/302022918

    I'd get about a 38A60-KVBE,...
  12. Replies
    22
    Views
    4,390

    lol

    lol
  13. Replies
    22
    Views
    4,390

    Hi, Hi, I think - inspect the caps for...

    Hi,

    Hi,

    I think - inspect the caps for bulging, end pops or leakage, and if they look OK carry on. If the start cap is cooked, then the drill won't start unless you give it an assist (careful...
  14. Replies
    6
    Views
    3,631

    Agreed, On looking around, nearly all the...

    Agreed,

    On looking around, nearly all the parallel port cards seem to be universal-type, 2 notches, 5V/3.3V. Reckon that would work OK? They are quite cheap anyway.

    Cheers

    PS No, wait,...
  15. Replies
    6
    Views
    3,631

    Thanks, It has indeed turned out to be...

    Thanks,

    It has indeed turned out to be electronic, being a faulty or below par parallel interface in the PC. On swapping the PC around, the problem disappeared, and the little machine seems to...
  16. Replies
    6
    Views
    3,631

    X and Y axis intermittent jamming

    Hi,

    We have a CNC 3020, on which the X and Y axis intermittently jam or stutter. The machine has had perhaps 40 hrs operation since new. The fault does not occur at the same spots in travel each...
  17. Replies
    4
    Views
    3,685

    Hi, Yes, I did previously see the jack oil. I...

    Hi,

    Yes, I did previously see the jack oil. I never mentioned that I need it for the headstock of a medium size lathe. Do you reckon that jack oil is an equivalent of Hyspin or similar? I had not...
  18. Replies
    4
    Views
    3,685

    Hydraulic oil ISO 32 - like Shell Tellus

    Hi,

    Anyone know of an outlet in Sydney towards Rockdale way, where I can readily buy ISO 32 hydraulic oil (eg Castrol Hyspin) in a 1L, 4L or 5L container, but not bigger?

    Ready supplies seem...
  19. Replies
    4
    Views
    3,178

    Thanks everyone, I am contacting these...

    Thanks everyone,

    I am contacting these companies.

    Cheers
  20. Replies
    4
    Views
    3,178

    Replacement lathe motor

    Hi,

    At our Men's Shed we have a Yangzhou lathe with a 1.5 kW single phase 4 pole motor which has died. It has a 100L frame which is odd in that rating, most 1.5 kW motors are 90L, a bit smaller....
  21. Replies
    22
    Views
    3,736

    Hi, If you do need to anneal it and reharden,...

    Hi,

    If you do need to anneal it and reharden, heat the key until it is bright red, and allow it to cool slowly, then drill. Then heat it to bright red again and quench it. After, with abrasive...