Search:

Type: Posts; User: Danbre Macase

Search: Search took 0.00 seconds.

  1. Replies
    2
    Views
    8,389

    Help with melting silver

    Hello. I was looking for some advice and info from people who actually know how to melt metals, hopefully you can help me. I am currently trying to melt some silver. I will be using an electric...
  2. Replies
    2
    Views
    7,615

    Thanks for the advice man. I will be careful not...

    Thanks for the advice man. I will be careful not to mix them together and will post it on the jewellery section.
  3. Replies
    2
    Views
    7,615

    Safely melting silver

    Hello. I was looking for some advice and info from people who actually know how to melt metals, hopefully you can help me. I am currently trying to melt some silver. I will be using an electric...
Results 1 to 3 of 3