24th Jan 2019, 07:49 PM
- Replies
- 31
- Views
- 10,790
So I'm pretty stoked with the outcome of my first...
So I'm pretty stoked with the outcome of my first welding project! I ended up returning the ozito welder and got a bossweld 150 amp M150. I'm really happy with it's performance and excited for my...
-
7th Jan 2019, 08:17 PM
- Replies
- 31
- Views
- 10,790
Thanks for your detailed advice Grahame! I picked...
Thanks for your detailed advice Grahame! I picked up some steel today from a local fabricator. All cut too size and reasonably priced! Keen to get practicing my welds.
Thanks again everyone. I'll... -
7th Jan 2019, 12:35 PM
- Replies
- 31
- Views
- 10,790
Thank you! That's a great idea. The mitres had me...
Thank you! That's a great idea. The mitres had me worried haha. Perfect solution and much more practical.
from Sunshine coast QLD -
6th Jan 2019, 10:26 AM
- Replies
- 31
- Views
- 10,790
Thanks for everybodys opinions. I'll let it all...
Thanks for everybodys opinions. I'll let it all soak in and then make a decision tonight.
I'm limited to buying only from bunnings for this. Please keep in mind i know they sell alot of junk in... -
5th Jan 2019, 11:27 AM
- Replies
- 31
- Views
- 10,790
Thanks alot! from Sunshine coast QLD
Thanks alot!
from Sunshine coast QLD -
5th Jan 2019, 09:05 AM
- Replies
- 31
- Views
- 10,790
Thanks for the advise. Excuse my lack of...
Thanks for the advise. Excuse my lack of knowledge in this field but is brazing like soldering?
from Sunshine coast QLD -
4th Jan 2019, 05:59 PM
- Replies
- 31
- Views
- 10,790
Thanks for all comments and suggestions! I've...
Thanks for all comments and suggestions!
I've tried to change my location but i can't figure it out for the life of me haha. I've put my location in my signature instead. I'm from Woombye, QLD.
... -
4th Jan 2019, 11:57 AM
- Replies
- 31
- Views
- 10,790
First time welding and wondering what I'm in for.
Hey everyone! So i posted on here a few months ago in relation to making coffee table legs out of flat bar steel 50mm by 5mm. Got some great advice and ended up investing in a universal bender. It...
-
16th Aug 2018, 05:31 PM
Thread: Table legs
by bradyofdoom- Replies
- 14
- Views
- 5,528
So here's my first attempt at the legs. I'm...
So here's my first attempt at the legs.
I'm really pleased with how they turned out! The universal bender was a very wise investment indeed. Extremely easy to use and had no trouble at all with... -
8th Aug 2018, 05:05 PM
Thread: Table legs
by bradyofdoom- Replies
- 14
- Views
- 5,528
I am able to do that. They've got a display one...
I am able to do that. They've got a display one in shop. I wasn't thinking it was gonna be easy haha. Metalwork has always kinda intimidated me. It's not as forgiving as woodwork haha!
I was... -
8th Aug 2018, 12:33 PM
Thread: Table legs
by bradyofdoom- Replies
- 14
- Views
- 5,528
Thanks for all replys and suggestions. I ended up...
Thanks for all replys and suggestions. I ended up going to a local mob for steel. I got 2 lengths at 1.3m 50×5mm.
Also going to invest in a universal bender from another local company for $230. ... -
7th Aug 2018, 09:20 AM
Thread: Table legs
by bradyofdoom- Replies
- 14
- Views
- 5,528
Thanks for the replys and suggestions. I did find...
Thanks for the replys and suggestions. I did find a local bloke making these but it was a bit too pricey, about $150 for the two. I figured I'd give it a crack myself.
I'm from Sunshine coast QLD... -
6th Aug 2018, 10:31 PM
Thread: Table legs
by bradyofdoom- Replies
- 14
- Views
- 5,528
Table legs
Gday everyone! First time poster and first time attempting metalwork. I do have experience in woodworking however.
I want to attemp to make some coffee table legs like these.
I will also be...