  1. PM China would George White be a good metal...

    PM
    China would George White be a good metal supplier.

    I ask because A&E meta only sells small pieces 300 x 300 and in thin 0.8mm stock.

    I need like 2 meters x 2 meters worth of copper, brass...
  2. Hi The three sided scraper is just a deburing...

    Hi

    The three sided scraper is just a deburing tool.

    We already have these - "hand shears for cutting sheet, files, safety glasses, ear protection, aprons, dust extraction"

    Okay 0.5 meters...
  3. Setting Up A Jewellery Workshop In A Secondary School

    I have been asked if to setup a Jewellery workshop in a secondary school. Making things like rings, necklaces and raise vessels. I did a sub major in Gold & Silver Smithing at uni but I have never...
  4. Replies
    40
    Views
    8,702

    Your 90% of the way home, good money in cider a...

    Your 90% of the way home, good money in cider a growth segment, more so in fruit spirits like schnapps if you can make quality product.
  5. Replies
    40
    Views
    8,702

    If I had access to an apple tree I would be...

    If I had access to an apple tree I would be making German Schnapps. Like my grandfather drank in his coffee back in the old country.
  6. Replies
    40
    Views
    8,702

    Like all things it's simple in practice and as...

    Like all things it's simple in practice and as difficult as you want to make it.

    Find someone local to hold your hand, a brew club, a brew store, a mate who can actually brew then jump in.
    ...
  7. Replies
    40
    Views
    8,702

    Cleaning heat exchangers are a pain. The standard...

    Cleaning heat exchangers are a pain. The standard way with dealing with it in brewing is to soak in caustic soda then flushed with water and then phosphoric acid rinse. This helps to clean any...
  8. Replies
    40
    Views
    8,702

    I do not have a lathe, if I did then yes I could...

    I do not have a lathe, if I did then yes I could do it. I am not the brains in this endeavour. The plans come from two blokes who are professional medicine men and I am simple doing what I am told. ...
  9. Replies
    40
    Views
    8,702

    Jack brewing beer is a great hobby, worst case is...

    Jack brewing beer is a great hobby, worst case is you make beer that gets you drunk, best case you make beer that makes you fly with flavours and aromas and then gets you drunk. :q

    The making of...
  10. Replies
    40
    Views
    8,702

    eskimo, pippin88 & PDW all ask good questions...

    eskimo, pippin88 & PDW all ask good questions however there is logic to this madness as most have not guessed this units full function.



    It's a closed system under pressure and temps up to 100...
  11. Replies
    40
    Views
    8,702

    That is such a cool idea. I never thought to use...

    That is such a cool idea. I never thought to use it for a domestic house. The only issue is it made with lead free solder, as it need to be food grade safe.

    The design is not as efficient as my...
  12. Replies
    40
    Views
    8,702

    The outer tube is 500mm long. Yes the inner tubes...

    The outer tube is 500mm long. Yes the inner tubes are welded first to the end plates and then the assembly is inserted into the 4" pipe.

    I can supply you with some of the 1/2" copper tube when I...
  13. Replies
    40
    Views
    8,702

    Micheal I have updated the drawing 377441 ...

    Micheal I have updated the drawing

    377441

    Okay lets go for 3mm plate at least 120mm x 120mm.

    Yes it will be TIG welded.

    Yes you are right the diameter of the plate is 98.34mm if we...
  14. Replies
    40
    Views
    8,702

    Will do

    Will do
  15. Replies
    40
    Views
    8,702

    Correct - home brewer

    Correct - home brewer
  16. Replies
    40
    Views
    8,702

    This is the copper pipe ...

    This is the copper pipe

    https://www.bunnings.com.au/kembla-1-2-x-1-5m-copper-straight-length_p4910028

    It says that its OD is 12.7mm.

    I planing to get the plate from George White |...
  17. Replies
    40
    Views
    8,702

    Hi Michael There is no need for high...

    Hi Michael

    There is no need for high precision.

    The placement of the holes just need to be the same in both plates (they need to align) however their exact position is not critical.

    Were I...
  18. Replies
    40
    Views
    8,702

    Can You Make These Two Copper Plates?

    I am a woodworker and I am not setup for metalwork so I am asking if anyone could machine two round copper plates for me. I am happy to reimburse you for your time and I can supply the copper for...
  19. Replies
    9
    Views
    2,678

    The tenon/spigot and the washer are a single...

    The tenon/spigot and the washer are a single piece and cannot be separated so that will not work. I also do not have a belt sander.
  20. Replies
    9
    Views
    2,678

    Knife Hinges Washer Re-machining

    I am building a small cabinet that has small 170mm high doors, I am using L-23 Brusso Offset knife hinges. However the washers on the hinges are to big 1.19mm for my small cabinet making the reveal...