Thanks for the reply ! (...
Thanks for the reply ! ( http://i.imgur.com/aYMaIjI.jpg )
this link is a picture of the jewellery (a brooch) that I've made, I have soldered both copper and brass together to create this funny... -
4th Oct 2016, 11:38 PM
- Replies
- 28
- Views
- 37,999
Need help !! about polishing soldered brass/copper jewelry.