23rd Jul 2018, 11:05 AM
Thread: Azstar mill tools
by WC57- Replies
- 4
- Views
- 10,933
Hi, just came across this post. Did you buy any?...
Hi, just came across this post. Did you buy any? I used them a lot while with a previous employer & they were very good. Cheers WC57
-
5th Dec 2016, 07:35 PM
Thread: Hardfacing question
by WC57- Replies
- 2
- Views
- 5,050
Thanks RC, the outer edges are still fine so I...
Thanks RC, the outer edges are still fine so I will do as you suggest & repair what is needed.
-
5th Dec 2016, 06:00 PM
Thread: Hardfacing question
by WC57- Replies
- 2
- Views
- 5,050
Hardfacing question
Hi, I have a loader bucket that has been hard faced before using a waffle pattern, but I don't know what sort of welding wire was used. It needs doing again & I would like to ask if it is ok to weld...
-
8th Oct 2016, 08:09 PM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
Well...I returned the machine to the seller for a...
Well...I returned the machine to the seller for a refund today & would like to thank everyone who offered help via this forum. Unfortunately I didn't have time to follow up on every lead as time was...
-
9th Sep 2016, 10:39 AM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
Very interesting, thanks Kryn. I will see how I...
Very interesting, thanks Kryn. I will see how I go getting hold of them...not giving up just yet.
Out of curiosity, what amps to you think this thing would draw? It came fitted with a 32amp 3... -
6th Sep 2016, 10:02 AM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
That's something else I was wondering...should...
That's something else I was wondering...should the pneumatic side of it work even if the ignitron tubes are faulty. No electrical diagrams are in the machine, Inductotherm are checking to see if they...
-
5th Sep 2016, 11:10 AM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
This welder is fitted with the Ignitron tubes...
This welder is fitted with the Ignitron tubes that are mentioned in the article on heat control which Michael G attached in an earlier response.
When the power is turned on, apart from a small... -
5th Sep 2016, 09:57 AM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
I thought I had updated this post...must not have...
I thought I had updated this post...must not have hit submit. Anyhow, the following is part of a the reply that I received from Inductotherm last week:
I am sorry to say, but I am not sure we can... -
27th Aug 2016, 07:00 PM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
Interesting articles Michael, very helpful if I...
Interesting articles Michael, very helpful if I ever get this thing going.
No joy with the sparky today, he needs a wiring diagram. We did establish that there is a closed circuit between the... -
27th Aug 2016, 10:25 AM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
Thanks Michael, very helpful information. I think...
Thanks Michael, very helpful information. I think you might be onto something with you comment regarding a contactor controlling welding current. Hopefully I will know more by the end of today....
-
26th Aug 2016, 09:18 PM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
Thanks Jekyll & Hyde, I traced the E Stop wires...
Thanks Jekyll & Hyde, I traced the E Stop wires back as far as I can go...they disappear into the main transformer somewhere. I have admitted defeat & have a sparky coming tomorrow morning to check...
-
26th Aug 2016, 11:37 AM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
Hi, I just spoke with Inductotherm & they appear...
Hi, I just spoke with Inductotherm & they appear genuinely interested in trying to help me out. Unfortunately one service guy is on his way back from overseas & the other is off sick today, but the...
-
26th Aug 2016, 07:58 AM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
Sure, I will try to attach a pic of the control...
Sure, I will try to attach a pic of the control panel here.
I did email Inductotherm on Tuesday but have not received a reply, I will ring them today. -
25th Aug 2016, 10:53 PM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
Thanks for the reply Stuart. I played around with...
Thanks for the reply Stuart. I played around with it a bit more today including adjusting the squeeze time knob down to zero...still no good. There is a red light that comes on inside the control box...
-
24th Aug 2016, 09:01 PM
Thread: Dorman spot welder help needed.
by WC57- Replies
- 24
- Views
- 6,499
Dorman spot welder help needed.
Hi, I have just acquired a used 30KVA Dorman spot welder & am having trouble getting it to work. It originally came from the ACT TAFE, fitting & machining section. The model no is 1/PS/201/C with...