Search:
Type: Posts; User: Com_VC
Search: Search took 0.02 seconds; generated 58 minute(s) ago.
-
1st Apr 2024, 05:19 PM
Thread: The hoisty thing
by Com_VC- Replies
- 9
- Views
- 733
SA Looks very similar to the Sky Hook. ...
Looks very similar to the Sky Hook.
https://www.machineryhouse.com.au/a358
Sent from my SM-N986B using Tapatalk -
13th Jan 2024, 08:56 AM
Thread: Brobo cold saw
by Com_VC- Replies
- 6
- Views
- 480
There would be no issue recouping your money, I...
There would be no issue recouping your money, I think you will end up getting more than what you paid for it.
Sent from my SM-N986B using Tapatalk -
13th Jan 2024, 02:33 AM
Thread: Brobo cold saw
by Com_VC- Replies
- 6
- Views
- 480
Well a non ferrous saw generally runs at 4000rpm,...
Well a non ferrous saw generally runs at 4000rpm, a proper cold saw for cutting steel is in the 40rpm range.
The filters and lines in your saw are not for running coolant, they are for the... -
12th Jan 2024, 08:39 PM
Thread: Brobo cold saw
by Com_VC- Replies
- 6
- Views
- 480
Are you only planning on using it for non ferrous...
Are you only planning on using it for non ferrous material such as aluminium or where you planning to cut steel with it?
It looks like a non ferrous saw from the photos but I could be wrong.
... -
6th Jan 2024, 06:16 PM
Thread: Another 'where to get?' thread- TPG stones
by Com_VC- Replies
- 8
- Views
- 716
Have you tried 3M cubitron sanding discs? They...
Have you tried 3M cubitron sanding discs? They are probably a lot more expensive than the Deerfos, but they last a long time!
https://www.3m.com.au/3M/en_AU/p/d/b40064724/
Sent from my SM-N986B... -
4th Jan 2024, 02:01 PM
- Replies
- 22
- Views
- 1,514
They also have the extra machinery bench grinder...
They also have the extra machinery bench grinder on sale for $198.
You could probably make up your own spindles and buy some buffing wheels.
https://www.machineryhouse.com.au/g159
Sent from... -
4th Jan 2024, 01:56 PM
- Replies
- 22
- Views
- 1,514
Machinery house have this, it says it weighs...
Machinery house have this, it says it weighs 69KG!
How can something powered by a 1HP motor be so heavy?
https://www.machineryhouse.com.au/g166
Sent from my SM-N986B using Tapatalk -
4th Jan 2024, 11:07 AM
Thread: Welding Helmet Lense
by Com_VC- Replies
- 8
- Views
- 945
Out of interest what helmet do you have? Might be...
Out of interest what helmet do you have? Might be time for an upgrade.
Sent from my SM-N986B using Tapatalk -
2nd Jan 2024, 08:44 PM
Thread: Wire Clamping Tool
by Com_VC- Replies
- 38
- Views
- 1,685
https://youtu.be/WxazYMD7a9s?si=5KqWU4DEVA_1PJKU...
https://youtu.be/WxazYMD7a9s?si=5KqWU4DEVA_1PJKU
Sent from my SM-N986B using Tapatalk -
2nd Jan 2024, 10:55 AM
Thread: Wire Clamping Tool
by Com_VC- Replies
- 38
- Views
- 1,685
I really should looking into getting both types,...
I really should looking into getting both types, not that they would ever get used much.
I have always just made it work with what I had available at the time, not the most efficient way though!
... -
2nd Jan 2024, 08:01 AM
Thread: Wire Clamping Tool
by Com_VC- Replies
- 38
- Views
- 1,685
Just found out the correct toom for these spring...
Just found out the correct toom for these spring clamps.
https://www.knipex.com/products/special-pliers/spring-hose-clamp-pliers/spring-hose-clamp-pliers/8551250AF
... -
1st Jan 2024, 11:04 PM
Thread: Wire Clamping Tool
by Com_VC- Replies
- 38
- Views
- 1,685
Do you have a photo of the special plier that is...
Do you have a photo of the special plier that is required for these as you mentioned earlier.
I've always just used pliers or vice grips as far as I can remember.
Sent from my SM-N986B using... -
1st Jan 2024, 01:11 PM
- Replies
- 27
- Views
- 3,453
Will a 240v ac powered inverter welder run from a...
Will a 240v ac powered inverter welder run from a dc supply?
Just an idea but with high voltage batterys such as the dewalt 60v now readily available, running 4 of them in series will give you 240... -
31st Dec 2023, 09:25 PM
Thread: Cashing in old car batterys, where to go?
by Com_VC- Replies
- 14
- Views
- 1,298
If I diluted the acid with water, would that make...
If I diluted the acid with water, would that make a good concrete cleaner?
Sent from my SM-N986B using Tapatalk -
31st Dec 2023, 05:23 PM
Thread: Cashing in old car batterys, where to go?
by Com_VC- Replies
- 14
- Views
- 1,298
Yeah $$$ in my account would be fine. Do I...
Yeah $$$ in my account would be fine.
Do I need an account or ABN etc
Would it be worth removing the lead myself, might get more $$$ worth that way or too much hassle?
Sent from my SM-N986B... -
31st Dec 2023, 02:19 PM
Thread: Cashing in old car batterys, where to go?
by Com_VC- Replies
- 14
- Views
- 1,298
Cashing in old car batterys, where to go?
Hi all,
Having a bit of a clean up whilst I am on holidays, I think I probably have around 10 old car batterys scattered around the place.
Is there anywhere I can take them for some cash, I... -
31st Dec 2023, 02:00 PM
Thread: Wire Clamping Tool
by Com_VC- Replies
- 38
- Views
- 1,685
I like how they are compact, I would like to know...
I like how they are compact, I would like to know if it would hold up for a permanent solution.
I'm not a fan of worm drive clamps, from experience I have seen leaks caused by them.
Lately I... -
28th Dec 2023, 06:29 PM
Thread: Need to weld this hole in my boat
by Com_VC- Replies
- 37
- Views
- 2,757
He mentions that he is using argon, as far as I...
He mentions that he is using argon, as far as I am aware there is no other option for TIG, well there are Argon/Helium blends but that would be for thicker materials, I have never seen it used...
-
So I changed the scale resolution to 10 micron...
So I changed the scale resolution to 10 micron and it is reading correctly now. It's now at 2 decimal points instead of 3, would that effect accuracy?
Good idea using the other output on the dro... -
22nd Dec 2023, 07:58 PM
Thread: Problems with UNIMIG Workshop 255
by Com_VC- Replies
- 7
- Views
- 730
Have you pulled out the liner? Make sure it's not...
Have you pulled out the liner? Make sure it's not damaged and you can easily feed the wire through without any restriction?
Also check that it is the right length. I was using a welder at work... -
22nd Dec 2023, 04:34 PM
Thread: Problems with UNIMIG Workshop 255
by Com_VC- Replies
- 7
- Views
- 730
Without actually striking an arc, maybe run the...
Without actually striking an arc, maybe run the wire speed at various speeds for say a minute each and see if you have consistent wire coming out.
On some welders 1-10 represents metres per... -
DRO Query
Hi all,
I have just a question about the dro that I am currently setting up on my lathe. I was expecting to be able to enter the diameter of the material but when I enter the diameter it doubles... -
12th Dec 2023, 05:55 AM
Thread: Magnetic DRO scale installation
by Com_VC- Replies
- 26
- Views
- 1,656
I figure extra protection shouldn't hurt. It only...
I figure extra protection shouldn't hurt. It only takes up about 1mm of usable travel space.
I'll grab some of that felt too, I should start looking into lead screw covers as well and possibly... -
11th Dec 2023, 06:25 PM
Thread: Magnetic DRO scale installation
by Com_VC- Replies
- 26
- Views
- 1,656
Where did you source the felt from, I'll add...
Where did you source the felt from, I'll add wipers down the track to the tail stock but for now I just added a stop to the crossslide using a m4 bolt, I probably should add wipers to the cross slide...
-
8th Dec 2023, 08:47 PM
Thread: Magnetic DRO scale installation
by Com_VC- Replies
- 26
- Views
- 1,656
Hi Dave, This is what I ended up with. I still...
Hi Dave,
This is what I ended up with. I still need to make up a stop in the carriage to protect it from the tail stock, will probably use an m5 or m6 cap screw.
Drill out 4 x 4mm holes to... -
5th Dec 2023, 05:41 PM
Thread: Magnetic DRO scale installation
by Com_VC- Replies
- 26
- Views
- 1,656
I found some 2mm aluminiun angle that should work...
I found some 2mm aluminiun angle that should work and some m3 countersunk torx headed screws. I was planning on using 2 screws maybe 10mm in from the ends, could possibly add a third in the middle if...
-
3rd Dec 2023, 11:16 PM
Thread: Magnetic DRO scale installation
by Com_VC- Replies
- 26
- Views
- 1,656
Those were my photos, was just playing around...
Those were my photos, was just playing around with it, glad you posted, it would have wasted a lot of space.
I am going to mount on the lathe chuck side of carriage, with some aluminium angle like... -
3rd Dec 2023, 12:54 PM
Thread: Magnetic DRO scale installation
by Com_VC- Replies
- 26
- Views
- 1,656
Hi Dave, here are some photos of how I was...
Hi Dave, here are some photos of how I was planning on mounting it, I'm glad you posted because I'd probably loose a lot of travel room for the tailstock.
Do you think it would be a big issue? I... -
1st Dec 2023, 07:57 PM
Thread: Magnetic DRO scale installation
by Com_VC- Replies
- 26
- Views
- 1,656
I just had a quick look at the lathe and mocked...
I just had a quick look at the lathe and mocked up how I am going to mount it all, looks like it will be a straight forward process.
I will try out the stick on straight to cross slide method for... -
1st Dec 2023, 06:25 PM
Thread: Magnetic DRO scale installation
by Com_VC- Replies
- 26
- Views
- 1,656
It's an MSR5000 read head, the magnetic tape is...
It's an MSR5000 read head, the magnetic tape is 10mm in width.
There is a machined surface on the cross slide for the tape to stick to. So if the adhesive fails, I can put some new adhesive on?
... -
1st Dec 2023, 09:31 AM
Thread: Magnetic DRO scale installation
by Com_VC- Replies
- 26
- Views
- 1,656
Magnetic DRO scale installation
Hi all,
I plan to install a magnetic scale to my cross slide due to limited space, I'll be using the magnetic tape.
Is there a installation guide available or does any one have any tips?
I... -
3rd Nov 2023, 02:55 PM
Thread: What did you learn today?
by Com_VC- Replies
- 940
- Views
- 592,338
Sticky: Something like this will probably do the job. ...
Something like this will probably do the job.
... -
21st Oct 2023, 05:22 PM
Thread: A belt untensioner?
by Com_VC- Replies
- 32
- Views
- 2,745
What about a new drill chuck? The type with a...
What about a new drill chuck? The type with a locking mechanism?
Sent from my SM-N986B using Tapatalk -
20th Oct 2023, 08:13 PM
Thread: A belt untensioner?
by Com_VC- Replies
- 32
- Views
- 2,745
So are saying the chuck opens up and the drill...
So are saying the chuck opens up and the drill bit falls out?
What size chuck it?
Sent from my SM-N986B using Tapatalk -
17th Oct 2023, 08:08 PM
Thread: What Respirator for spray painting
by Com_VC- Replies
- 8
- Views
- 5,654
Think it comes with cartridges, whether they are...
Think it comes with cartridges, whether they are the right type for paint fumes, I'm not sure.
Had a quick look on aliexpress and plenty of parts around, filters you can get 5 pairs for $50.
... -
17th Oct 2023, 07:50 AM
Thread: What Respirator for spray painting
by Com_VC- Replies
- 8
- Views
- 5,654
What about something like this, looks to be good...
What about something like this, looks to be good value at $30, I had a look at an equivalent from a shop and they run at about $400.
Apparently can be converted to air feed to do 2k.
... -
16th Oct 2023, 06:46 PM
Thread: What Respirator for spray painting
by Com_VC- Replies
- 8
- Views
- 5,654
What Respirator for spray painting
Hi all,
I plan to do a bit of spray painting in the future, mainly just small jobs with oil based enamel but also considering using iso based 2k due to it being harder wearing.
So just looking... -
10th Oct 2023, 09:00 PM
Thread: how is this profile shape made
by Com_VC- Replies
- 7
- Views
- 1,148
I would say they would be roll formed. Sent...
I would say they would be roll formed.
Sent from my SM-N986B using Tapatalk -
8th Oct 2023, 03:55 PM
Thread: Thread Dial Indicator
by Com_VC- Replies
- 31
- Views
- 2,365
Anyone found a good DIY ELS solution, I'm...
Anyone found a good DIY ELS solution, I'm seriously considering it and I reckon I have all the parts required scattered around the house/garage somewhere [emoji3]
Sent from my SM-N986B using... -
6th Oct 2023, 05:38 PM
Thread: Rod Bender 3mm - 6mm
by Com_VC- Replies
- 4
- Views
- 660
Thanks for the link/suggestions, a few good ideas...
Thanks for the link/suggestions, a few good ideas there.
Just found this one too, looks fairly easy to replicate.
https://restosupplies.co.nz/rod-bender
Sent from my SM-N986B using Tapatalk -
4th Oct 2023, 09:10 PM
Thread: Rod Bender 3mm - 6mm
by Com_VC- Replies
- 4
- Views
- 660
Rod Bender 3mm - 6mm
So I would like the ability to make some hooks, most likely the type to use on a pegboard.
So would like to know what bender would be the most suitable for this.
I'd even consider a homemade... -
4th Oct 2023, 06:18 PM
Thread: Cannot access thread
by Com_VC- Replies
- 2
- Views
- 1,156
OK thanks, waiting longer worked, I need to be...
OK thanks, waiting longer worked, I need to be more patient next time [emoji3]
Sent from my SM-N986B using Tapatalk -
4th Oct 2023, 12:24 PM
Thread: Cannot access thread
by Com_VC- Replies
- 2
- Views
- 1,156
Cannot access thread
Hi,
I am having trouble accessing the Sieg Z Axis thread, it was working yesterday at some point, now it just says "Loading" and nothing happens.
I can access all other threads without any... -
21st Sep 2023, 06:18 PM
Thread: Plasma Cutter Glasses
by Com_VC- Replies
- 8
- Views
- 887
I just used to use shade 5 glasses, same type you...
I just used to use shade 5 glasses, same type you would use when using oxy/acetylene.
Sent from my SM-N986B using Tapatalk -
11th Sep 2023, 08:34 PM
Thread: Tube bender suggestions
by Com_VC- Replies
- 33
- Views
- 2,496
I was planning on making a JD2 type bender at...
I was planning on making a JD2 type bender at some stage, they seem to be a common thing in the fabrication industry but not sure if it would suit your requirements.
... -
11th Sep 2023, 08:29 PM
Thread: Tube bender suggestions
by Com_VC- Replies
- 33
- Views
- 2,496
What about a 3 phase motor and vfd, you should be...
What about a 3 phase motor and vfd, you should be able to program that to stop pretty quickly.
Sent from my SM-N986B using Tapatalk -
3rd Sep 2023, 10:07 PM
Thread: Small Tube Benders
by Com_VC- Replies
- 38
- Views
- 2,956
I have the black one, I never had any issues with...
I have the black one, I never had any issues with it.
You can get this type as well but it is 1/4" minimum.
... -
3rd Sep 2023, 08:18 PM
- Replies
- 1
- Views
- 730
Sheraton 9" AM thread cutting, am I missing a gear?
Hi all,
I need to cut an M24 x 1.5 thread, I've never really done much thread cutting on a lathe in the past as I thought it was too much effort and went out and bought a die or tap to suit.
So... -
1st Sep 2023, 07:25 PM
Thread: What air fitting is this?
by Com_VC- Replies
- 11
- Views
- 1,365
Worth checking out cejn as well, it looks...
Worth checking out cejn as well, it looks similar.
Sent from my SM-N986B using Tapatalk -
21st Aug 2023, 07:07 AM
Thread: The effect of lubrication !
by Com_VC- Replies
- 10
- Views
- 925
I once read that water is the best cutting fluid,...
I once read that water is the best cutting fluid, the downside, it causes rust.
Sent from my SM-N986B using Tapatalk