Refers to an old Scripta engravers pantograph currently used for miling aluminium and brass. Every time I switch it on during wet/humid weather it trips the circuit breaker. Leave it in the sun for a while on a sunny day and it's back in operation. Any suggestions about cause/repair/way around? :)