Hi everyone,
I'm after some Sodium Silicate to make sand cores but I am trying to find somewhere I can get some from.
An earlier post mentioned that the sodium silicate from a pottery supplier does not work as well as proper Sodium Silicate for casting. Has anyone had experience with this and could someone let me know where I could get hold of some?
Thank you