I recently bought a CK Flex Loc torch with one piece cable from Weldfabulous in the US. I've now done a good few 8 hours days worth of solid welding with the torch and thought I'd provide feedback for anyone who may be looking for a new torch.
I've very happy with the torch and the cable is a delight to use. It's not water cooled so I do need to be careful when working at high currents. In a few cases I've had to stop mid weld as my fingers have been getting too toasty. Generally however for a home shop it would be fine I think, I didn't want the hassles of a water cooler and don't do too much aluminium. I can however appreciate the advantages of water cooling and it's a little frustrating to stop mid stream. The one piece cable is super flexible and an absolute delight to use.
This is the torch
TIG welding torches from CK Worldwide Quality TIG Welding Torches & Accessories
I happened to have my phone in the workshop today, so took a couple of quick snaps of my own torch and the last weld I did before stopping for a cuppa. That was some 4 mm SHS and 5 mm (IIRC) flat plate. Welding at max 150 amps.
Needless to say, no connection with any company mentioned, etc., just happy customer
Pete
http://i738.photobucket.com/albums/x...lding/file.jpg
http://i738.photobucket.com/albums/x...ing/file-1.jpg