Needs Pictures: 0
Results 1 to 9 of 9
Thread: Casting Anvils
-
27th Nov 2018, 10:07 AM #1
Casting Anvils
I started this journey with making a small wooden split pattern but couldn’t figured a good way to do my logo and the text. Sometime later I got a Aldi 3D Printer.
So I downloaded Fusion 360 and got to learning on the fly and 3D modeled my anvil with draft.
First print using sample filament that came with the printer hence color changes as it ran out.
I printed a whole bunch more for economics it’s cheaper to have 8 in a mould than individually ram each one up.
Had a fixed flask dimension and had to try to work out how many I could fit into the flask and where the sprue, runners, gates etc would be.
I sprayed all the prints with high build spray putty and hand sanded them all back with wet n dry paper. I didn’t want any of the print layers showing through.
I drew up a template for the flask and drilled the location pins.
The match plate all rammed up gives this sand mould in the flask.
After pouring in bronze.
…..Live a Quiet Life & Work with your Hands
-
27th Nov 2018, 10:39 AM #2Golden Member
- Join Date
- Dec 2011
- Location
- Sydney
- Posts
- 505
Congratulations!
A great demo of design to print to casting. What metal?
Cheers
Bill
-
27th Nov 2018, 10:40 AM #3
Damn iv’e lost the second post.
I did Bronze, Brass, and SG Iron.…..Live a Quiet Life & Work with your Hands
-
27th Nov 2018, 10:49 AM #4
The next step was a side step as I had to rebuild the mill to finish the anvils. That can be seen in another thread.
Basic clean up of the flashing. 24 Minis, 8 of each Metal.
Milled the base and then the tops.
Followed this up with some wire wheeling, filing, and a scotch brute fine wheel.
20 finished, the 4 remaining will be kept to pass on to my Daughter.
These were meant to go on to my market stall this weekend at Yarra Glen. But I have nearly sold out in one day I have 1 SG Iron, 2 Bronze and 5 Brass left. That’s what I get for showing them on Facebook.
Some even went to collectors in USA and Australia. Allocating anvils to orders and packaging and posting.
…..Live a Quiet Life & Work with your Hands
-
27th Nov 2018, 06:25 PM #5
Very nice. Out of interest, what are they selling for?
-
27th Nov 2018, 06:27 PM #6
$60ea for Brass & SG Iron, $70 Bronze.
…..Live a Quiet Life & Work with your Hands
-
28th Nov 2018, 09:17 AM #7Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,255
beautiful work DSEL
-
28th Nov 2018, 01:28 PM #8China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,656
Can I have the SG posted to SA at my cost
-
28th Nov 2018, 01:30 PM #9
Similar Threads
-
Anvils
By Bob47 in forum THE SMITHYReplies: 8Last Post: 27th Feb 2013, 07:26 PM -
Anvils?
By Aerohydro in forum THE SMITHYReplies: 36Last Post: 11th Nov 2012, 11:16 PM -
Casting about for cast iron casting ideas
By Graziano in forum THE FOUNDRYReplies: 49Last Post: 1st Apr 2012, 12:05 PM -
Anvils for sale- SE Qld.
By Andy Mac in forum METALWORK GENERALReplies: 0Last Post: 25th Oct 2008, 12:45 PM -
Anvils
By Marc in forum METALWORK GENERALReplies: 2Last Post: 28th Sep 2007, 06:38 PM