    I bought some hole saws at an auction and this set of gadgets was included in the lot. After serious efforts to work out what they're used for we gave up. Does anyone have any idea?

  2. #2
    Join Date
    Feb 2007
    Location
    Katherine ,Northern Territory
    Age
    69
    Posts
    736

    Default

    Quote Originally Posted by Rossluck View Post
    I bought some hole saws at an auction and this set of gadgets was included in the lot. After serious efforts to work out what they're used for we gave up. Does anyone have any idea?

    First pic looks like a collet chuck of some description .
    Third pic ,the thing with the ball bearings in it is a tube swage ,it rolls the the raised collar on the tubes you have with the tools .

    Looks like it maybe a radiator repairers tool for making hose necks .

    Kev.
    "Outside of a dog a book is man's best friend ,inside a dog it's too dark to read"
    Groucho Marx

  3. #3
    Join Date
    Jun 2006
    Location
    Vic
    Posts
    5,631

    Default

    They're used for putting the raised section on the tube as pictured with the short bits of tubes.

    You put them in the end of the appropriate sized tube and then screw them up so that the ball bearings roll the impression in the tube
    Cheers

    DJ


    ​ADMIN

  4. #4
    Join Date
    Dec 2005
    Location
    Gold Coast
    Age
    66
    Posts
    192

    Default

    Brilliant. Thanks. I had no idea.