Thanks Thanks:  0
Likes Likes:  0
Needs Pictures Needs Pictures:  0
Picture(s) thanks Picture(s) thanks:  0
Results 1 to 10 of 10
  1. #1
    Join Date
    Jan 2006
    Location
    Malvern East
    Posts
    36

    Default How should I treat exposed steel?

    I am curently rebuilding a trailer and it has a bit of surface rust on it. I have just finished removing the metal floor from it and as a result grinded nearly all cross members down to the steel.

    What should I use to prepare the steel ready for paint?

    For the moment I have just hit it with some gloss black paint I had lying around.

    Brenton

  2. #2
    Join Date
    Jul 2006
    Location
    Canberra
    Age
    54
    Posts
    883

    Default

    Not that I know much about metalworking but I would be inclined to use some sort of rust inhibiter...

    Along the lines of galmet. It can be sprayed or brushed on and works well.

    Pete

  3. #3
    Join Date
    May 2005
    Location
    Turramurra, NSW
    Posts
    66

    Default

    Provided it's bright steel and no rust left, I really like the bitumised paints. They are also soft, so that any metal you overlay has a bit of a cushion. Unfortunately it takes 2 weeks to fully dry and your chioce of next coats is limited.

    Alternately Cold Gal, always assuming there's no rust
    Bodgy
    "Is it not enough simply to be able to appreciate the beauty of the garden without it being necessary to believe that there are faeries at the bottom of it? " Douglas Adams

  4. #4
    Join Date
    Oct 2001
    Location
    Warwick, QLD
    Age
    45
    Posts
    1,165

    Default

    Use something like "KillRust Cold Galvit".

    The paint contains stuff that inhibits the further development of rust and the galvanic components protect from future rust. Make sure that you give it a really nice thick coat on all components (including mating surfaces) before you put the floor in. Then slop some more on the weld areas after the floor has gone back in.
    Have a nice day - Cheers

  5. #5
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by BrentonSpear
    For the moment I have just hit it with some gloss black paint I had lying around.
    Pity about that because you should have rust inhibited first. Now if you want to do it properly you will have to remove the paint. No amount of stuff you apply over the paint will fix this problem. The first bit of paint that chips (or any tiny holes you left unpainted) lets in the air and it is probably rusting as we speak!

    A cheap rust inhibitor is dilute phosphoric acid, it turns red rust into iron phosphate (blue) and when it dries you can paint right over that. I would recommend stripping off the gloss paint and using a proprietary rust inhibitor and then some decent paint. That galvit stuff that wood butcher describes is also top stuff.

  6. #6
    Join Date
    Feb 2006
    Location
    Melbourne
    Age
    65
    Posts
    316

    Default

    Hi,

    Here is the info pertaining to the "GALVIT" stuff.

    http://www.wattyl.com.au/Specifiers/...ils.htm?Id=387

    & here is the site for the "GALMET" stuff. There is also a FAQ section.

    http://www.galmet.com.au/driver.asp?page=main/home

    Regards
    David

  7. #7
    Join Date
    May 2003
    Location
    Kuranda, paradise, North Qld
    Age
    62
    Posts
    65

    Default

    Once you've finished treating all the steel, consider putting in a ply floor instead of steel. Makes for a quieter trailer and guaranteed not to rust! . I've had a sheet of 15mm exterior hardwood ply in the trailer that I built more than 6 years ago and it's still sound. It should see out ten years and only gets a coat or two of decking oil every year or so). Glue it in place with a cartridge of sikaflex and a handful of rivets or teks. It will be a lot easier to replace than a steel floor too.

    Mick
    "If you need a machine today and don't buy it,

    tomorrow you will have paid for it and not have it."

    - Henry Ford 1938

  8. #8
    Join Date
    Aug 2003
    Location
    .
    Posts
    1,175

    Default

    How should I treat exposed steel?

    Take it to a movie, have dinner together, but it flowers.

    Al

  9. #9
    Join Date
    Apr 2004
    Location
    Werribee, Vic
    Age
    66
    Posts
    539

    Default

    How long does it flower for?

  10. #10
    Join Date
    Dec 2005
    Location
    Gold Coast
    Age
    66
    Posts
    192

    Default

    Quote Originally Posted by BobL
    Pity about that because you should have rust inhibited first. Now if you want to do it properly you will have to remove the paint. No amount of stuff you apply over the paint will fix this problem. The first bit of paint that chips (or any tiny holes you left unpainted) lets in the air and it is probably rusting as we speak!

    A cheap rust inhibitor is dilute phosphoric acid, it turns red rust into iron phosphate (blue) and when it dries you can paint right over that. I would recommend stripping off the gloss paint and using a proprietary rust inhibitor and then some decent paint. That galvit stuff that wood butcher describes is also top stuff.
    This is the best advice. (1) You unfortunately have to remove all of that black paint. (2) Wipe over with some rust remover (this neutralises the rust in the pits that you can't see) , clean it off, (3) hit it with a good metal primer, (4) then you can paint it with anything.

Similar Threads

  1. Welding question ? ... Is this dangerous ?
    By JDarvall in forum WELDING
    Replies: 36
    Last Post: 9th Mar 2006, 12:29 PM
  2. Corrugated steel strips: Where to buy? How to make?
    By Peter Dow in forum METALWORK GENERAL
    Replies: 6
    Last Post: 20th Jun 2005, 10:28 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •