A few months back Joe put up a small power hacksaw for sale
//metalworkforums.com/f223/t203...-power-hacksaw
Which I managed to snag. Partly bought for curiosity, but also occasionally I fabricate with stainless steel and the bandsaw does not like that at all, so I revert to a hacksaw or angle grinder to cut it.
A couple of people who missed out asked for details, so -
As the label says, it is a 'Peerless' product, made back in the early 1980's.
P1040596.JPG P1040597.JPG
The vice is pretty standard and can hold something 130mm high by 140mm wide (maximum). Based on that I would suggest 100mm square. It looks like it might be designed to take slippers to make mitre cuts.
P1040598.JPG
The blade fitted is a 10" blade, but with some shuffling it could take a 12" blade (I think). Back end is just a couple of screws, front has a tensioning device of sorts. Horrible to get to that back screw though.
P1040603.JPG P1040604.JPG P1040599.JPG
The cutting action is through a motor, geared down and then driving a scotch yoke like device. My tacho suggests around 160 strokes per minute (60mm stroke).
P1040601.JPG
Original paint is indeed a bright green hammer tone
P1040605.JPG
It runs, although I haven't tried it on metal yet. First up it needs to be cleaned and lubricated. Worth noting that whenever getting secondhand electrical equipment that looks to have not been used for some time - check the wiring. Opened up the plug to check and both the active and earth pulled out of the screw terminals very easily.
Michael
-
10th Jun 2019, 08:00 AM #2Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
-
23rd Jun 2019, 08:56 PM #3Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
I was going to clean it first, but the temptation with 5 minutes to knock off was too strong.
P1040611.JPG
Cuts nicely, and faster than I can with a hacksaw. Next to no shaking of the table it was on as well.
Michael
Similar Threads
-
Help With Power Hacksaw
By stevo81 in forum METALWORK GENERALReplies: 14Last Post: 21st Mar 2017, 11:55 AM -
Power hacksaw
By morrisman in forum ANTIQUE AND VINTAGE MACHINERYReplies: 1Last Post: 16th Jul 2016, 11:07 PM -
power hacksaw ID
By dodge at4 in forum ANTIQUE AND VINTAGE MACHINERYReplies: 2Last Post: 9th Jun 2016, 02:13 PM -
Power Hacksaw
By Auskart in forum METALWORK GENERALReplies: 4Last Post: 4th Sep 2011, 09:37 PM -
SOLD: power hacksaw
By mistercartoon in forum METALWORK - Machinery, Equipment, MARKETReplies: 2Last Post: 19th Mar 2011, 05:51 PM