Hi all .. I need to reproduce this nut for a vintage vice I am working on.. thread diameter is 7/8" or 22.2 mm.. pitch is just over 4 turns to the inch..
a couple of questions,.. because of the mystery number of turns.. how would you set up your lathe to cut this thread ?
secondly... as it is brass, would it be possible to cast the nut around the screw, using the screw as a mandrel ??
Like all projects, is it going to be worth the effort in the long run..
Ken.
-
20th May 2019, 02:28 PM #2Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
I would say it will absolutely be 4 TPI, it'll just be wear making it hard to tell. Is it a square form or ACME? Screw cutting without knowing the exact pitch is impossible.
Sent from my Nokia 8 Sirocco using Tapatalk
-
20th May 2019, 03:19 PM #3Senior Member
- Join Date
- Jul 2010
- Location
- Brisbane
- Posts
- 143
-
20th May 2019, 03:39 PM #4Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
I think you have a 4tpi thread where someone has messed up or the machine was totally worn that made it, what brand is the vice? I'd probably just make a new screw and nut, screw cutting that pitch will be hard.
Sent from my Nokia 8 Sirocco using Tapatalk
-
20th May 2019, 07:20 PM #5Most Valued Member
- Join Date
- Aug 2008
- Location
- Charlestown NSW
- Age
- 65
- Posts
- 1,673
-
20th May 2019, 07:23 PM #6Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Rather than trying to make sense out of the nut, measure the very end of the thread. Usually that will be the least worn bit and give you the best idea.
Casting around the screw is unlikely to work well. A nut that size will single point quite nicely.
Added: just looked at my lathe thread chart. It has 4 1/2 and 4 3/4 listed too - would one of those fit better?
Michael
-
20th May 2019, 08:00 PM #7Golden Member
- Join Date
- Jun 2007
- Location
- Vic
- Age
- 48
- Posts
- 544
or count the thread/turn over 2->3", even 4" that will give better accuracy?
-
21st May 2019, 11:41 AM #8Senior Member
- Join Date
- Jul 2010
- Location
- Brisbane
- Posts
- 143
-
21st May 2019, 07:22 PM #9Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Maybe set the screw up in your lathe, set the pitch for 6mm and using a piece of wood or something marked with a square thread profile, see if that 6mm pitch holds all the way along. If you get to the end and the sides of the 'cutter' look to line up (allowing for wear), that might help see whether it is metric.
Michael
-
21st May 2019, 07:28 PM #10Most Valued Member
- Join Date
- Apr 2012
- Location
- Healesville
- Posts
- 2,129
Put the screw in your lathe and set the feed to 4 tpi and your lowest rpm, set a tool up just as a pointer and then run the lathe in the air so to speak, and see if the pointer follows the thread all the way to the end.
If it does then your first problem is solved.
cheers, shed
-
21st May 2019, 07:31 PM #11Most Valued Member
- Join Date
- Aug 2008
- Location
- Charlestown NSW
- Age
- 65
- Posts
- 1,673
-
21st May 2019, 07:36 PM #12Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
I would be very, very surprised if any vice needing a rebuild and sold here was metric. I'd be verging on hat eating territory.
Sent from my Nokia 8 Sirocco using Tapatalk
-
21st May 2019, 07:43 PM #13Senior Member
- Join Date
- May 2019
- Location
- Picnic Point, Sydney
- Age
- 77
- Posts
- 314
Count the number of threads over a longer distance on the lead screw, say 150 or 6". If it's 6mm pitch you'll count 25 over the 150mm and imperial 1/4" then the count will be 24 over the 6".
Which ever one it is won't be easy. You could always make a tap too.
Similar Threads
-
Restoration Projects - Tough Drill Press - Dawn Drill Press - Record Pipe Vice
By bwal74 in forum METALWORK - Machinery, Equipment, MARKETReplies: 0Last Post: 10th Feb 2019, 03:11 PM -
carter no 4 vice , pipe vice,triton saw holder
By robyn2839 in forum METALWORK - Machinery, Equipment, MARKETReplies: 1Last Post: 27th Nov 2018, 04:27 PM -
Vice Stop ( or why the vice is still not painted Michael )
By Anorak Bob in forum METALWORK GENERALReplies: 4Last Post: 5th Jan 2016, 09:01 PM -
Shaper vice and milling vice
By morrisman in forum METALWORK GENERALReplies: 6Last Post: 5th Sep 2012, 12:06 AM -
260 restoration
By Finnowa in forum THE HERCUS AREAReplies: 7Last Post: 18th Oct 2010, 12:14 AM