    Quote Originally Posted by phaser View Post
    Question :
    What is the best, most forgiving type of parting tool ?
    As a novice, using a 9 inch Hercus, my learning is that a rigidly mounted blade is essential... and the only way it has worked for me is a rear mounted tool (upside down as mentioned) on a T slot cross slide. This has parted steel on Dad's lathe with little stress on me.
    Any attempt to use a front mounted parting blade on Ali or steel is definately something I will not repeat.
    Brass has been fine.
    So what ever tool and holder, rigidity is number one... Then of course, on centre and sharp and appropriate lube.
    cheers
    David

    ------------------------------------------------
    A society grows great when old men plant trees whose shade they’ll never sit in. (Greek proverb)

  2. #17
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    35
    Posts
    1,522

    Default

    Quote Originally Posted by Dave J View Post
    That looks great, but he does have a rigid machine.
    Always wondered why the factory supplied carbide parting tips don't come sharpened with the right side higher, so the part comes off first nice and flat and the nib is left on the stock and removed after the part has left.
    I always sharpen my HSS this way.
    Most of my carbide parting tips are formed with the right side slightly higher and further forward, most of them are taegutec.

  3. #18
    Join Date
    Jan 2019
    Location
    Adelaide
    Posts
    78

  4. #19
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by caskwarrior View Post
    Most of my carbide parting tips are formed with the right side slightly higher and further forward, most of them are taegutec.
    Never have known that, good to know thanks. The one I have from many years ago is straight.
    Using Tapatalk

  5. #20
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    Quote Originally Posted by 4me View Post
    I bought one of those a while back.
    It leaves an aweful rough surface on the face so no good..

  6. #21
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    Quote Originally Posted by Dave J View Post
    Never have known that, good to know thanks. The one I have from many years ago is straight.
    I have 2 or 3 already HSS tools that are sharpened that way but they don't have much of a reach. I can only part small stuff with them and so I need one that will go a lot further.

  7. #22
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    I know my mini lathe is 8mm tool height but my AL350A is something weird like 14 or 16 mm. I'll have to check.

  8. #23
    Join Date
    Jan 2019
    Location
    Adelaide
    Posts
    78

    Default

    Quote Originally Posted by phaser View Post
    I bought one of those a while back.
    It leaves an aweful rough surface on the face so no good..
    Yes, one surface is rough the other a lot better, I guess it comes down to making sure the blade is lined up perfectly with the cross slide. I don't worry about it so much just face the rough end.

  9. #24
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    Quote Originally Posted by 4me View Post
    Yes, one surface is rough the other a lot better, I guess it comes down to making sure the blade is lined up perfectly with the cross slide. I don't worry about it so much just face the rough end.
    No both surfaces end up very rough and with pitting and galling.

  10. #25
    Join Date
    Jun 2007
    Location
    sydney ( st marys )
    Age
    64
    Posts
    4,890

    Default

    The tool may not be sharpened correctly or set correctly or there maybe an issue with machine ridgidity, is the tool cutting through the material okay or are you hearing or feeling a binding sound, are you parting with feed and using coolant, what material are you parting,and if under power what diameter, speed and feed are you using.
    Is the tool set up to part close to the chuck?
    Do you have minimal over hang of the tool?

  11. #26
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    The AL350A has a tool height of 18mm.

  12. #27
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Tubal Cain,the American one, AKA Mr Pete has a U Tube video.

    https://www.youtube.com/watch?v=w0N6K9y2i2M

    It reinforces many comments made here, but worth watching.

    Grahame

  13. #28
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    Quote Originally Posted by pipeclay View Post
    The tool may not be sharpened correctly or set correctly or there maybe an issue with machine ridgidity, is the tool cutting through the material okay or are you hearing or feeling a binding sound, are you parting with feed and using coolant, what material are you parting,and if under power what diameter, speed and feed are you using.
    Is the tool set up to part close to the chuck?
    Do you have minimal over hang of the tool?
    I'll see if I can get a photo of the tool tomorrow.

  14. #29
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    I already had a few of these blades in a bundle of stuff from a garage sale but not tested then until now. The tool holder came from china (ebay).
    From memory it was 32mm aluminium I tried to part and it mangled both parting faces. Could hear the binding as it cut.
    I don't believe there's any rigidity problem. It's a pretty solid lathe.
    I always use WD40 or Inox on aluminium and always part as close to the chuck as I can get.
    Can't use power feed at the moment as the lathe needs a new gear, teeth mashed a bit on the 40T.
    It did have a bit of overhang by design of the tool, prob around 35mm to the tool tip.

    I think I tried it on steel too hence the tool needs resharpening now.

    The first picture depicts the blade profile before grinding.







  15. #30
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    The top surface is the wrong shape. You need to grind it flat.


    Sent from my iPad using Tapatalk
    Chris

Page 2 of 3 FirstFirst 123 LastLast

Similar Threads

  1. parting tool geometry
    By brendanh in forum METALWORK GENERAL
    Replies: 19
    Last Post: 25th May 2015, 06:58 PM
  2. Replies: 19
    Last Post: 19th Mar 2014, 02:29 PM
  3. Parting off tool ?
    By morrisman in forum METALWORK GENERAL
    Replies: 5
    Last Post: 10th Oct 2013, 11:36 AM
  4. Your best parting tool
    By iron bark in forum METALWORK GENERAL
    Replies: 61
    Last Post: 20th Dec 2012, 07:40 PM
  5. Parting tool mounted on rear tool post advice needed
    By colbra in forum METALWORK GENERAL
    Replies: 17
    Last Post: 12th Feb 2012, 02:49 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •