Is that from Ozemestore, in Pt Adelaide???? If it is, good luck keeping an edge on the "HSS"
I found it was only marginally better than Mild Steel, unless they've got it from a different supplier.
I put anything from that place in the same category as their lathes and mills, CRAP, would be the only thing that comes to mind that's allowed on this Forum.
KrynTo grow old is mandatory, growing up is optional.
-
13th Apr 2019, 12:16 AM #62Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Bugger, any idea's where to order the hss blank tools? Hare and forbes does a 3 pack but they are 8mm my machine takes 6mm that is a far amount of grinding
-
13th Apr 2019, 12:31 AM #63Senior Member
- Join Date
- Oct 2015
- Location
- melbourne
- Posts
- 473
https://www.machineryhouse.com.au/L0003
Is 1/4. Pretty close to 6mm
Also have other sizes from 1/8"
Russ
-
13th Apr 2019, 12:46 AM #64Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Thanks Russ from memory i bought a pack of the 8mm before for my toy aluminium lathe so i dont know if they were ok says on h&f made in India, India is a poor country but do they actually make a quality product? I'm thinking China quality here but please correct me
Cant really compare my toy machine to my mini machine 24watt motor to 250watt motor so the toy lathe would never blunt a tool in its whole life
-
13th Apr 2019, 02:28 AM #65
Hi Gazza, Guys,
Gazza I know you are keen to make chips, but take a few moments to consider what you have and what you need. I've collected much of the HSS cutting tools I have, from scrap bins, scrap yards, old drills and broken taps, all very useful. Buying a grinder is the first step to making your own lathe tools. That chart that Dave posted is a very useful one. At a glance you can see the tool shape that you need for a particular cut ! Avoid using carbide your lathe really doesn't have the power to usefully use them.
Having to use shims can get to be a pain in the neck, I know because that is what I used to do. I would collect a stack of shims for a particular tool and fasten them together with an elastic band !
Not any more I made a Norman Patent tool holder for my lathe, and wish I had made one years ago. No more prating about with shims. I did a write up a while back, its on here somewhere. You can make it to use any size tool blank. Mine is 1/2" inch, 13 mm if you want metric.
To go with that a proper grinding rest for your grinder and then you can grind your tools accurately. Search for Harold Hall, he has a lot of very useful things on his web site, including the grinding rest.
Whilst I remember, the parting tool only needs to stick out just over half the diameter of the work. If its too big to part then get the hacksaw out and clean off on the lathe with a facing cut. Don't try and part to a depth of more than three times the blade width. A 1/2" blade 1.5" inches deep.
Lots and lots to learn it takes time.Best Regards:
Baron J.
-
13th Apr 2019, 02:52 AM #66Golden Member
- Join Date
- Dec 2007
- Location
- Adelaide
- Posts
- 574
I've got one of those Supercheap $30 grinders and in all honesty I would not recommend getting one as your main grinder - they are quite under powered and bog down very quickly once you put a bit of pressure on the wheel to shape the tool, they are really only good for touching up a slightly blunt tool and twist drills, my main grinder is a 200mm grinder and this is the one I use for lathe tools I only use the small one to touchup a tool that has lost it's edge. If you keep an eye on gumtree you will eventually pick up a used half decent grinder for around the same price, I would not go below 150mm.
-
13th Apr 2019, 10:48 AM #67Most Valued Member
- Join Date
- Jun 2011
- Location
- Australia east coast
- Age
- 71
- Posts
- 2,713
-
13th Apr 2019, 11:22 AM #68
Here are some on ebay already sharpened and ready to go. If you buy these you can see how there sharpened and copy on other HSS blanks.
If I remember right, this seller always sold good gearUsing Tapatalk
-
13th Apr 2019, 02:43 PM #69Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
I went to super cheap to pick up one of those $30 bench grinders i think it works ok u need to be putting a fair amount of force on the hss tool to slow the motor right down and than the little hss tool heats up within 7 seconds and needs a dip but bloody hell is it repetitive i was there forever trying to make a new tool i got the and just extended one of the cut off tools that came with my lathe and i resharpened it
i just remade the first wheel spacer and with my hole drilling in the center i just missed my sixteen mil depth by about 1.5mm bugger!!! so once i cut the part off i was left with the back over the wheel spacer which i had to put back in the lathe other way around and dicked it, it is still usable just not a 100 percent good finish about a 80 percent effort i ...... up again hopefully wont do it again
here is the first right to left tool i cut from a new piece of hss i bought from hare and forbes these hss bits seem to be ok it didn't go blunt it stayed very sharp after i was finished, the tool is laying on its side its actually a right to left tool i need to make a left to right one soon for facing
the other pictures show i had 19mm stick out of the cut off tool, my tools are six mm (number six doesn't work on my keyboard) so 3 times the stick out 18mm i went over by 1mm, it shows the cut off tool cut right thru almost 28mm thickness of material i had next to no chatter because i took the advice from you guys and kept the tool close to the chuck
-
13th Apr 2019, 03:38 PM #70Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
You can see the difference with using a decent HSS.
Welcome to a long learning curve of machining.
KrynTo grow old is mandatory, growing up is optional.
-
13th Apr 2019, 04:17 PM #71Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
That wheel spacer in those last pictures on the tail stock was a bad cut it was one i done yesterday or the day before and turned it around put it back into the chuck i'll show todays effort when i do one more
getting really tired of remembering numbers not as in annoying but as in repeating the dial number so i know how much to take off on the next pass if its not to the zero
think i need to put calipers on the lathe
-
13th Apr 2019, 04:37 PM #72
It doesn't look like you have much back rake, if you look in the picture of HSS bits I posted you can see they all have it. With more back rake it shaves the material off like a chisel, aluminum especially likes more back rake.
Using Tapatalk
-
13th Apr 2019, 06:29 PM #73Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
This afternoon's effort is done i buggered that small piece the aluminum kept pulling out of the chuck while i was facing it not sure why i had 1:1 in the chuck and what was hanging out i had to drill my center hole than go up in drill bit size than come back to finish facing it once it had minimal amount of face left on the aluminium i tried using the tool cross to the bed and inline with the bed both methods kept chucking the job out of the chuck i still dont know which way to face but i manage
tomorrow are the last 3 pieces how will i cut 39mm deep into that one long piece with only a six mm tool? do u think i should machine it down to OD size than cut it off to length place it back in the chuck than try machine the hole? what will be the best way i have no clue hope you guys can offer advice
Thanks Dave i will take a look at some more pictures and see where i can improve i know i have a lot to learn about making the tools
-
13th Apr 2019, 07:20 PM #74Banned
- Join Date
- Jan 2019
- Location
- Adelaide
- Posts
- 78
Save your money and buy an AL-50, better known internationally as a 9x20. Good small lathe and they pop up frequently second hand on Gumtree.
-
13th Apr 2019, 07:24 PM #75Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
4me your shout? There is nothing wrong with my lathe i spent 4 hours on it this afternoon absolutly mad little machine its doing everything i ask of it or expect it to do
Similar Threads
-
Mini Lathe
By Mutawintji in forum METALWORK GENERALReplies: 32Last Post: 25th Apr 2013, 01:35 PM -
SOLD: The Mini Lathe
By Big Shed in forum METALWORK - Machinery, Equipment, MARKETReplies: 1Last Post: 30th Jan 2011, 10:23 AM -
Mini Lathe
By elderly in forum METALWORK GENERALReplies: 12Last Post: 1st Dec 2010, 09:21 PM -
Mini Lathe
By dj_pnevans in forum METALWORK GENERALReplies: 1Last Post: 22nd Apr 2010, 11:46 PM -
Mini Lathe
By Bodgy in forum METALWORK GENERALReplies: 6Last Post: 6th Aug 2005, 11:50 PM