Went to visit a friend recently who was preparing to do some offset turning. He needed to make the following part out of a pump on an old tractor. The part was no longer available. The smaller pin had broken off flush with the base and he had welded it back but was not happy with the join so decided to make it from one piece.
This is the piece to be made. Looks ok here after welding but Stuart felt the join was too weak.IMG_1484.jpgIMG_1485.jpg
IMG_1488.jpg He drew up a plan before starting.
Preparing the setup to begin machining. The steel bar is 2 1/2 " in size IMG_1486.jpg IMG_1487.jpg IMG_1489.jpg IMG_1490.jpg
IMG_1507.jpg I forgot to take some photos during the machining as the concentration level was high but here is the finished piece.
This sort of work is so time consuming. Looking at the initial failure, failed trial of welding, drawing up plans to machine, preparation prior to machining (cutting stock to size, marking up with a high level of precision, center drilling, loading faceplate on lathe, finding an appropriate size lathe dog, checking that the lathe tool will miss everything during machining), careful machining with lots of measuring, grinding the centre plate to size and drilling the two holes to finish. Stuart does it as a challenge and generally does not charge anything for his time. Anyway it was a good learning day for me and I really enjoyed it.
Cheers
Mark
-
18th Mar 2019, 06:08 PM #2Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,227
Brings back memories. About 8-9 years ago at work, we were doing a lot of parts for stamping presses, including crankshafts. It got to the point where it was a novelty to machine parts concentric. I don't miss doing that work, its something that takes a lot of skill to pull off well.
-
18th Mar 2019, 08:02 PM #3
Hi Mark, Guys,
Nice job !
That is an ideal job for an independent four jaw chuck. A lot less hassle than setting up between centres.Best Regards:
Baron J.
Similar Threads
-
Dawn Offset Vice
By doily_grunge in forum GENERAL DISCUSSION / OFF TOPICReplies: 3Last Post: 28th Nov 2017, 04:52 PM -
Offset Dawn Vice Repair
By wm460 in forum METALWORK GENERALReplies: 37Last Post: 8th Nov 2014, 11:08 PM -
offset boring head for wood?
By jack620 in forum METALWORK GENERALReplies: 10Last Post: 28th Apr 2010, 10:32 PM -
Calculating cam offset in a 3 jaw
By Tiger in forum METALWORK GENERALReplies: 0Last Post: 15th Mar 2010, 09:59 PM -
Offset needed for cam in a 3 jaw chuck
By Tiger in forum METALWORK GENERALReplies: 13Last Post: 8th Oct 2009, 04:28 PM