Thanks Thanks:  0
Needs Pictures Needs Pictures:  0
Picture(s) thanks Picture(s) thanks:  0
Results 1 to 5 of 5

Thread: heating

  1. #1
    Join Date
    Apr 2014
    Location
    Perth
    Posts
    134

    Default heating

    hi
    will a propane gas bottle with a heating torch give enough heat to bend
    a 50x8 mm bar at right angles
    cheers steve

  2. #2
    Join Date
    Oct 2015
    Location
    melbourne
    Posts
    473

    Default

    Maybe, if you can arrange some firebrick to minimise the heat loss.
    Depends on how tight the bend radius is.
    And how long the piece is, to get leverage.


    Russ

  3. #3
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,658

    Default

    Also will depend on the burner size

  4. #4
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    charcoal will do it..it will take a while to get it red hot and a fan assisted charcoal bed will be hotter

  5. #5
    Join Date
    Aug 2015
    Location
    Melbourne, Australia
    Posts
    843

    Default

    If it is the bunnings type then they struggle to make anything truly hot - maybe hot enough for helping press stuff in out of other parts etc but *really* hot - nope.

    I keep a few red bricks dry and out of the weather so that if I need to heat something as best I can I arrange them and the piece such that the heat doesn't escape too much.

    Greg.

Similar Threads

  1. Oxy/LPG. Heating Tip
    By DSEL74 in forum WELDING
    Replies: 8
    Last Post: 20th Feb 2018, 09:31 PM
  2. Heating Oil - moved from Foundry
    By Turbine Builder in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 4
    Last Post: 28th Jan 2018, 09:54 PM
  3. Oxy heating tip vs welding tip
    By Matt_M in forum METALWORK GENERAL
    Replies: 5
    Last Post: 11th Jan 2015, 06:31 PM
  4. LPG heating torches
    By shedhappens in forum METALWORK GENERAL
    Replies: 67
    Last Post: 31st Aug 2012, 10:36 PM
  5. Heating jig
    By Tiger in forum METALWORK GENERAL