Hi everybody,
Happy new year to you all.
I am looking for advice on what type of felt would be suitable for a surface grinder spindle that runs on plain bearings. And who might supply it.
I did get some from a local supplier in Melbourne and it looked good, but it it is full of very fine grit and the fibres just seem to go everywhere - so not that great for a low clearance spindle. Not their fault really - this is at the extreme end of what felt might be expected to do I guess.
So I figuring it has to be very high quality, very clean, and a tight structure.
All help / advice appreciated.
Greg.
-
4th Jan 2019, 08:18 PM #2Most Valued Member
- Join Date
- Apr 2012
- Location
- Healesville
- Posts
- 2,129
G/day Stray, i have bought felt from spotlight and they had quite a few types and thicknesses to choose from.
cheers shed
-
4th Jan 2019, 08:26 PM #3Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Probably closer to the mark would be the felt they use for piano repairs, as you want a high quality felt. I was able to buy some felt here in Adelaide some years back. I think the place is called 'Felt Fabricating', in Edwardstown. They sold by the metre from rolls 900mm wide and up. If you only want a small piece I may have some left over.
Michael
-
4th Jan 2019, 09:39 PM #4Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Hi there,
Not sure what thickness of felt you are after but I have bought engineering felt on ebay on several occasions. Here is an example:
https://www.ebay.com.au/itm/FELT-Eng...2JLx:rk:3:pf:0
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
4th Jan 2019, 10:54 PM #5Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
Try the bearing suppliers.
-
4th Jan 2019, 11:47 PM #6China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Phone for Felt Fabricating PTY Ltd : (08) 8374 1429
-
5th Jan 2019, 02:29 AM #7
Hi Greg,
I've used billiard baize before now as oil wicks behind unshielded ball races in electric motors. There is a pool table supplier quite local to me who will throw out loads of the trimmings when they refurbish a table. The only difficulty is that it is very hard to cut it accurately without a pair of punches and because it is quite thin ( couple of mm ) you need three or more rings to get any thickness.Best Regards:
Baron J.
-
5th Jan 2019, 10:17 AM #8Golden Member
- Join Date
- Aug 2015
- Location
- Melbourne, Australia
- Posts
- 843
Wow, thank you all. That is quite some replies. Appreciated.
It is not just getting hold of some felt - but knowing the correct felt for this particular application. It is a very specific application I guess. There are many different engineering grades available (https://www.mcmaster.com/felt) and some better than others for very low viscosity oil like I am using (kero). Also things like high flow wicking, and compressibility (as the tolerences are very tight). Seems maybe the F5 type that mcmaster carr sells is the one - dunno (?).
JJ Davies seems to the local people here. That is where i got the felt I have presently. I believed it was engineering felt I got, but maybe that was not the case. And I didn't ask after the grade when I got it a while back. Interestingly, it is a 'sandwich' - that is the top and bottom of it seems to be made of a different (more pure) material than the 'filler'.
Everybody was on hols still this week so I'll contact Davies and the crew in SA as well (thanks for the details) next week. I'll post here with what I learn.
Thanks again,
Greg.
EDIT: It seems in Oz we have 'A' and 'B' grade engineering felts. Some interesting spiel here: A Grade Engineering Felt - Associated Gaskets. It doesn't seem very standardised though. Their A grade felt is 95% wool. These people have an A grade that is 70% wool ... https://www.swiftsupplies.com.au/a-g...ndustrial-felt
-
5th Jan 2019, 10:35 AM #9.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
Hi Greg,
Looks like you have a number of possible sources, here is another - Felt Sales PTY LTD
Felt.JPG
Bob.
-
5th Jan 2019, 10:39 AM #10Golden Member
- Join Date
- Aug 2015
- Location
- Melbourne, Australia
- Posts
- 843
Thanks Bob. Seems they are about - sadly not too many of them say their products are 'suitable for 3000rpm spindle applications with 3 micron tolerance running oil that feels like water'. I wish they did!! )
I think I might just have to get some grades and see how they feel.
-
5th Jan 2019, 09:19 PM #11Member
- Join Date
- Dec 2014
- Location
- melbourne
- Posts
- 72
G'day, you might try J.J.Davies & Sons 1299 North Road Huntingdale. They have a large range of felts of all sorts.
-
5th Jan 2019, 10:53 PM #12Golden Member
- Join Date
- Aug 2015
- Location
- Melbourne, Australia
- Posts
- 843
Thanks shedeng, yep - that is where I got my current felt. With the grit and bits of wood in it. It was an off cut so who know what I ended up getting. I'll contact them this week.
Similar Threads
-
Lathe felt
By TheNutter in forum METALWORK GENERALReplies: 11Last Post: 11th Aug 2015, 10:01 AM -
Felt for Lathe Way wipes
By argeng in forum METALWORK GENERALReplies: 9Last Post: 2nd Jun 2013, 11:11 AM -
Need a tool and cutter grinder or plans thereof
By Kentower in forum METALWORK GENERALReplies: 12Last Post: 29th May 2010, 10:56 PM -
Engineering Felt
By Lanza_1 in forum METALWORK GENERALReplies: 8Last Post: 7th Nov 2009, 09:51 PM -
Posts, or the lack thereof
By LineLefty in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACKReplies: 15Last Post: 11th Aug 2004, 10:15 PM