    The bloke I help out from time to time is looking at getting a plate roller. Have seen one that has the roll diameter of 110 and a width of 1870. The bottom rollers appear to be very close together, with the top roller above the centre of the 2 bottom rollers.
    Would anyone know what capacity this machine could be? The seller doesn't know the capacity, as he only buys and sells used equipment.
    Have attached an image for better reference.plate roller.JPG
    Thanks in Advance.
    Kryn
    To grow old is mandatory, growing up is optional.

  2. #2
    Join Date
    Aug 2011
    Location
    Perth, Western Australia
    Age
    67
    Posts
    362

    Default

    4 mm maybe up to 6 mm.

  3. #3
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    Comparing the build strength of the components to that of a pan brake, I would have thought maybe 2mm or less, at full width. Maybe slightly thicker with reduce width.

    If I were to guess, I would say it was a sheet roller, not a plate roller.

    Simon
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  4. #4
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Just looked on Hare and Forbes site, there 4mm one is 2m x 150 roller. And there 2.5mm one is 2m x 150 roller.
    It looks like that one would be 2mm max, maybe 1.6 at full width
    Using Tapatalk

  5. #5
    Join Date
    Oct 2008
    Location
    N.W.Tasmania
    Posts
    1,407

    Default

    It will depend a lot on what hw wants to roll. There will be almost an order of magnitude difference between some stainless steel sheet materials and say soft aluminium sheets or copper sheet. It may be able to roll 8mm of pure aluminium plate, but something as tough as Bisalloy would be another matter altogether. For those tough materials the limit could be under 1mm for a full width sheet.

  6. #6
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    It's far too light to be a plate roll. Definitely a sheet roller.

    I would guess at full width no more than 3mm or 4mm sheet thickness.

  7. #7
    Join Date
    Apr 2008
    Location
    Perth
    Posts
    269

    Default

    Agree with everyone, thats a tiddler, used for light thin sheet. Plate rollers are big bastard 3 phase machines with tremendious hydraulic strength to roll plate.

    DD

  8. #8
    Join Date
    Aug 2011
    Location
    Perth, Western Australia
    Age
    67
    Posts
    362

    Default

    I have to admit I know nothing of which I speak.
    Out and about today I had a conversation with a gentlemen I use to work with back in the day. After being told that my memory sucks he reminded me that the machine we used had 6" rollers, was heavy framed and struggled with 6 mm.

    So I retract my 4 mm may be 6 mm comment.

    He suggests, (as others have done) that its probably a sheet roller up to 3 mm.

    Tony

  9. #9
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    Thanks everyone for the replies.
    I found out today, that what he's looking for is something 2400+ wide and capable of rolling 5mm steel, minimum!!!
    He could have told me that before I went looking
    Kryn
    To grow old is mandatory, growing up is optional.

  10. #10
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by KBs PensNmore View Post
    Thanks everyone for the replies.
    I found out today, that what he's looking for is something 2400+ wide and capable of rolling 5mm steel, minimum!!!
    He could have told me that before I went looking
    Kryn
    That's going to be one heavy machine, I hope he has the power supply up to it.
    Using Tapatalk

  11. #11
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    I find Google is my friend to help out with the unknown, this time I googled Hare and Forbes plate rolls and found they get big real quickly for plate, they don't even supply rolls for the really big stuff.
    Quote Originally Posted by bts View Post
    I have to admit I know nothing of which I speak.
    Out and about today I had a conversation with a gentlemen I use to work with back in the day. After being told that my memory sucks he reminded me that the machine we used had 6" rollers, was heavy framed and struggled with 6 mm.

    So I retract my 4 mm may be 6 mm comment.

    He suggests, (as others have done) that its probably a sheet roller up to 3 mm.

    Tony
    Using Tapatalk

  12. #12
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    Thanks for that Dave, didn't realise they sold them. Not too bad a price for Chinese made, he'll be running it off a 65kva Generator, if the CNC Plasma cutter's not being used, as I don't think it'll run both of them.
    Kryn
    To grow old is mandatory, growing up is optional.

  13. #13
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by KBs PensNmore View Post
    Thanks for that Dave, didn't realise they sold them. Not too bad a price for Chinese made, he'll be running it off a 65kva Generator, if the CNC Plasma cutter's not being used, as I don't think it'll run both of them.
    Kryn
    Machines4u is another one, many new and second hand ones available Australia wide.
    Using Tapatalk

  14. #14
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Default

    Hi Kryn,

    I agree with previous posts, definitely a sheet roller, 2.5 mm tops at that width.

    I have a small 18" wide set of rolls, It maxes out at 1.5 mm in steel and 2 mm in alloy. Even rolling 12" wide copper into a 100 mm cylinder is hard work on the handle.
    Best Regards:
    Baron J.

Similar Threads

  1. Rolling rings from 8mm rod
    By Scally in forum METALWORK GENERAL
    Replies: 13
    Last Post: 1st Jan 2017, 08:13 PM
  2. Rolling copper
    By denncarm in forum METALWORK GENERAL
    Replies: 5
    Last Post: 27th Oct 2013, 05:15 PM
  3. Rolling Tailstock Arbor
    By barkersegg in forum METALWORK GENERAL
    Replies: 5
    Last Post: 9th Dec 2011, 08:22 AM
  4. Rolling brass plate
    By SHIPPERS in forum METALWORK GENERAL
    Replies: 0
    Last Post: 23rd Oct 2009, 06:04 PM
  5. rolling metal tubes
    By piobuilleann in forum METALWORK GENERAL
    Replies: 2
    Last Post: 29th Jun 2007, 05:22 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •