    Default

    Sikaflex automotive windscreen adhesive is the go here I believe.

  2. #17
    Join Date
    Dec 2010
    Location
    Syd
    Posts
    492

    Default

    You might find the various 3m scotchweld products over there more available. Hysol is another specific aluminium bonding epoxy , but unless using it a fair bit, smallest quantity is like a quart tin.

  3. #18
    Join Date
    Feb 2003
    Location
    formerly from Sydney (north of The Harbour), NSW, Oz
    Age
    68
    Posts
    306

    Default

    Quote Originally Posted by Michael G View Post
    He's in Canada guys - they don't have Bunnings there
    but they do have Home Deport, Rona and Lowes -- he should be able to find Sikaflex in one of them
    regards from Canmore

    ian

Page 2 of 2 FirstFirst 12

Similar Threads

  1. Joining Aluminum Tubing
    By aagui in forum WELDING
    Replies: 16
    Last Post: 18th Jan 2017, 09:15 PM
  2. Tapering or coupling aluminum tubing
    By horseatingweeds in forum METALWORK GENERAL
    Replies: 22
    Last Post: 13th Oct 2016, 09:12 AM
  3. aluminum arc welding
    By johnyjamtin in forum WELDING
    Replies: 6
    Last Post: 22nd May 2014, 12:59 AM
  4. Aluminum
    By benupton in forum METALWORK GENERAL
    Replies: 5
    Last Post: 1st Apr 2010, 01:11 AM
  5. Aluminum Solder
    By Nurgle in forum METALWORK GENERAL
    Replies: 7
    Last Post: 2nd Aug 2007, 12:46 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •