    Default Sorry, another "What metal is best" thread

    I want to make a few more toolholders as shown. 25 x 36 x 69 size and extremely hard. I have a set of Japanese Hardness Tester files, bought from Japan but through ebay(?) and none of them will mark the existing holders. Does that mean the hardness is >RC65 or that the files are carp! HRS is the only steel readily available locally so, being low carbon, would that limit me to case hardening only for the new ones?

    Image2.jpgImage3.jpgImage1.jpg

    As before, suggestions would be appreciated. Thanks

    Charles

  2. #2
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    35
    Posts
    1,522

    Default

    Case hardening these is absolutely fine. They definitely don't need to be 65rc, the only places that would benefit from hardening is the little v way and the retaining slot.

  3. #3
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Not even sure I would be bothered hardening them if they are only for home shop use.

    Michael

  4. #4
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    I didn't bother hardening any of mine.
    The ones I've used have held up fine in a home shop environment.
    Making Dickson style quick change tool post holders (picture heavy)
    Using Tapatalk

  5. #5
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Default

    Hi Guys,

    I see "Photobucket" is getting into using your pictures for advertising !
    Best Regards:
    Baron J.

  6. #6
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    35
    Posts
    1,522

    Default

    Hy Dave, great thread there. I'd ask this there but it's closed, how is the blackening holding up on the adjusters you did? Have you filled all the holders?

  7. #7
    Join Date
    Apr 2015
    Location
    Tungkillo, South Australia
    Age
    87
    Posts
    74

    Default

    Thanks for the help, guys.

  8. #8
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by caskwarrior View Post
    Hy Dave, great thread there. I'd ask this there but it's closed, how is the blackening holding up on the adjusters you did? Have you filled all the holders?
    The blackening has held up great, and on many other thing I have done also.
    No haven't got anywhere near filling them.
    I moved house's 5 times in 7 years just after making them, so now I'm permanently settled again I can set more up.
    Using Tapatalk

  9. #9
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by BaronJ View Post
    Hi Guys,

    I see "Photobucket" is getting into using your pictures for advertising !
    I just looked but didn't see any.
    Maybe because I'm logged into it all the time.
    Using Tapatalk

  10. #10
    Join Date
    Jun 2011
    Location
    Australia east coast
    Age
    71
    Posts
    2,713

    Default

    Quote Originally Posted by Michael G View Post
    Not even sure I would be bothered hardening them if they are only for home shop use.

    Michael
    This. I never hardened the ones I made and I'm pretty sure they'll be functional a lot longer than I will.

    PDW

  11. #11
    Join Date
    Aug 2009
    Location
    East Warburton, Vic
    Posts
    357

    Default

    Quote Originally Posted by Dave J View Post
    I just looked but didn't see any.
    Maybe because I'm logged into it all the time.
    1F2CDA1F-6B31-4575-8B77-D67A2039A862.png
    Cheers

    DJ

  12. #12
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    I doesn't come up like that for me, maybe because I'm always logged into photo bucket, not sure.
    Using Tapatalk

  13. #13
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Default

    Well that make s sense ! They wouldn't want you to know that they were taking advantage of your pictures, now would they !
    Best Regards:
    Baron J.

  14. #14
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by BaronJ View Post
    Well that make s sense ! They wouldn't want you to know that they were taking advantage of your pictures, now would they !
    Hahaha that's true
    Using Tapatalk

Similar Threads

  1. M34 X 2.5 "Special Metric Thread" Hand Tap
    By glivo in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 0
    Last Post: 4th Jul 2018, 12:37 PM
  2. Problems Accessing Thread - "This web page has a redirect loop"
    By RoyG in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACK
    Replies: 5
    Last Post: 13th Jul 2014, 12:04 AM
  3. New Thread Title to Replace "today's tool gloat"
    By Oldneweng in forum METALWORK GENERAL
    Replies: 104
    Last Post: 7th Jun 2014, 03:58 PM
  4. Replies: 5
    Last Post: 28th Jan 2014, 09:47 PM
  5. WEST AUST Hercus metal lathe 12" x 42" excellent condition
    By craig manley in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 0
    Last Post: 6th Jul 2011, 02:29 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •