5th Oct 2018, 12:37 AM #1Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,038
No mess cast iron
I repurposed an old cast iron hub from the scrap pile (post#143 in Tips and Tricks). I call it cast iron because it was definitely a cast item, it was ferrous, and there was a piece broken out of it typical of damaged cast iron. My past experience of turning cast iron is that I end up looking like an underground coal miner, but that wasn't the case with turning this hub.
The metal was coming off the tool in a typical shower of tiny chips but they were clean, there was no horrible black dust.
I'm thinking the hub must have been made from a low carbon cast iron. Or looking at it the other way a steel with extra carbon to lower the melting temp and increase the fluidity for casting, I have read of 'semi-steel cast iron' in advertising blurbs. Any thoughts?
IMG_1991.jpg
IMG_1992.jpg
-
5th Oct 2018, 12:42 AM #2
Hi Bob,
Looking at those chips, I would say that was cast steel. The surface grain looks to fine to be iron.Best Regards:
Baron J.
-
5th Oct 2018, 08:38 AM #3Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
The chips look the same as those I got from some 4E cast iron bar I machined recently, but the finish on the workpiece is much shinier.
Chris
-
5th Oct 2018, 06:25 PM #4Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,225
Looks like SG iron.
-
5th Oct 2018, 06:41 PM #5Senior Member
- Join Date
- Nov 2008
- Location
- Sydney
- Posts
- 112
I concur.
Chas.
Similar Threads
-
When does cast iron not machine like cas t iron?
By simonl in forum METALWORK GENERALReplies: 20Last Post: 31st Jul 2018, 08:57 PM -
Cast Iron
By Auskart in forum METALWORK GENERALReplies: 9Last Post: 28th Jul 2017, 06:08 PM -
Cast iron fireplace - Question for restoring using Penetrol & Liberon Iron Paste
By mookschank in forum METALWORK GENERALReplies: 8Last Post: 19th Jun 2013, 06:32 PM -
Cast iron VS Cast steel lathe compound slide
By Ueee in forum METALWORK GENERALReplies: 10Last Post: 23rd Dec 2012, 11:40 PM -
Cast Iron
By RayG in forum METALWORK GENERALReplies: 17Last Post: 30th Apr 2011, 02:27 PM