Lathe chuck back plate
Hi there, I am purchasing a new chuck for my metal lathe, I will have to make a new back plate, is there any reason why it can't be made from aluminium( I have some good aluminium stock) instead of cast or steel, which I don't have any off, has anyone made one from aluminium or think of any reason why it can't be done, I would appreciate any ideas or advice.
Regards
Nick
-
28th Aug 2018, 11:39 PM #2Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
No reason why it can't be done , it will work.
Reasons why it shouldn't be done, it is soft,will mark and bruise easily,if it is a threaded back plate the threads may get damaged by screwing on/off the rear register face may wear quite quickly if it is put on and off often.
-
29th Aug 2018, 01:07 AM #3Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
A while ago I bought some cast iron backplate castings (as cast, unfinished) that I’m never going to use, I think they are 200 OD but I’ll have to check. PM me if you think one of those would be useful.
-
30th Aug 2018, 12:35 AM #4
Hi Guys,
Small bar bell weights from the scrap yard are a good source of cast iron for this purpose. I have a couple of 2kg ones stashed away, about 150 mm X 25 mm thick at the rim and centre. They would probably give about 12 or 13 mm thickness when the lettering has been skimmed off. The hub is nearly 65 mm diameter, so should provide plenty of meat for the register.Best Regards:
Baron J.
Similar Threads
-
hercus ,qualos lathe face plate and chuck back plates
By KBs PensNmore in forum METALWORK - Machinery, Equipment, MARKETReplies: 4Last Post: 7th May 2017, 02:13 PM -
spare D-4 back plate for 8" chuck
By thorens in forum METALWORK GENERALReplies: 4Last Post: 26th Nov 2013, 09:08 PM -
Chuck back plate
By morrisman in forum METALWORK GENERALReplies: 38Last Post: 15th Dec 2011, 07:17 PM -
chuck back plate thread
By tanii51 in forum THE HERCUS AREAReplies: 13Last Post: 10th Jun 2011, 11:36 PM -
Lathe D1-3 Chuck Mounting Plate
By electrosteam in forum METALWORK - Machinery, Equipment, MARKETReplies: 2Last Post: 29th Jul 2010, 05:44 PM