Not quite Michael. They can be forged from pipe by a blacksmith. Start with the major diameter then draw it out and taper it to length and minor diameter.
But we still dont understand the finished design are the tentacles purely decorative or are they partially or fully structural? Makes a big difference to the possible methods of manufacture.
They could be solid forged steel, hollow forged, fabricated, cast, made out of something other than metal and sprayed with metal mist.
Not enough info supplied.…..Live a Quiet Life & Work with your Hands
Similar Threads
-
Line boring dingo loader arms
By .RC. in forum METALWORK GENERALReplies: 35Last Post: 16th Nov 2015, 07:48 AM -
Roller Rocker or Airbags with Trailing Arms - What's best?
By simonhogg1 in forum TRAILERS & OTHER FABRICATED STUFFReplies: 7Last Post: 21st Mar 2014, 04:00 PM -
Birmingham Small Arms Company Limited - lathe chuck
By nearnexus in forum METALWORK GENERALReplies: 5Last Post: 19th Oct 2013, 08:56 AM