    Round head.. more rounded than dome head I believe... cheese head would be fine also.. depends what is avail
    Attached Images Attached Images

  2. #17
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Quote Originally Posted by BaronJ View Post
    Now since 3/32" is almost spot on for 7BA, you could use that size.
    Quote Originally Posted by nadroj View Post
    The USA thread 3-48 ASME is another alternative.It's 5.25 thou larger in diameter, but has the same 48 tpi as 3/32 BSW.
    It would be good to have an alternative size in case he doesn't have the 3/32 BSW. The above two posts are in conflict though. According to Google 7BA is 52.92 tpi.
    Chris

  3. #18
    Join Date
    Jul 2010
    Location
    Brisbane
    Posts
    143

    Default

    Quote Originally Posted by jack620 View Post
    It would be good to have an alternative size in case he doesn't have the 3/32 BSW. The above two posts are in conflict though. According to Google 7BA is 52.92 tpi.
    3-48 would suffice.
    Ken

  4. #19
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    No joy, sorry Ken. The closest they had was 3-48 cap screws in black.


    Sent from my iPhone using Tapatalk
    Chris

  5. #20
    Join Date
    Nov 2008
    Location
    Perth WA
    Age
    71
    Posts
    6,459

    Default

    Quote Originally Posted by kenny_10 View Post
    Hi all..

    .. to make it more difficult, they have to be bright !

    Ken in Bris.
    Hello Ken,

    If the fixings are only available zinc plated then the zinc can be readily removed with phosphoric acid. BobL, our resident chemist ( amongst other titles ), put me onto Chemtech Rust-Off which has a higher concentration of acid than most other over the counter concoctions. Available from Bunnings and works very effectively at converting those garishly plated fixings to sombre "bright" steel.

    https://www.bunnings.com.au/chemtech...mover_p1107356

    Bob.

  6. #21
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    A search of a few UK-based screw suppliers leads me to suspect these things are unobtainable. Making them might be your only option Ken.
    Chris

  7. #22
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,481

    Default

    Hi Chris, Guys,

    Quote Originally Posted by jack620 View Post
    It would be good to have an alternative size in case he doesn't have the 3/32 BSW. The above two posts are in conflict though. According to Google 7BA is 52.92 tpi.
    My error ! I looked at diameter and didn't check twice... Sorry for any confusion.
    Best Regards:
    Baron J.

Page 2 of 2 FirstFirst 12

Similar Threads

  1. small steel round head slotted wood screws #2, #3, & #4
    By eskimo in forum METALWORK GENERAL
    Replies: 28
    Last Post: 26th Nov 2013, 09:08 PM
  2. Small UNC/UNF machine screws
    By Ueee in forum METALWORK GENERAL
    Replies: 10
    Last Post: 13th Nov 2013, 09:15 PM
  3. Sourcing Aluminium Hex Rod
    By Chris Parks in forum METALWORK GENERAL
    Replies: 8
    Last Post: 23rd Apr 2013, 10:57 PM
  4. Online supplier of small screws
    By snowyskiesau in forum METALWORK GENERAL
    Replies: 26
    Last Post: 20th Sep 2010, 03:00 PM
  5. New Website for Sourcing Stuff in Oz
    By hux in forum METALWORK GENERAL
    Replies: 3
    Last Post: 19th Jan 2008, 11:03 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •