    I am interested in making some home made 250-202 QCTP tool holders. I would be looking to make 3 or 4 of them and was wondering:

    1) Where would I get steel to suit? I think I would need a piece 30mm thick by 90mm wide x 200mm long to make four. I would be able to mill the dovetail in one go with a piece like this.
    2) Could they be made out of aluminium? I could cast the bar required that way.
    3) would this be economically viable given they could be bought new for $45 each delivered? I imagine the steel off the shelf would be very expensive.

    Grateful for any thoughts or suggestions.

    Brendan

  2. #2
    Join Date
    Apr 2018
    Location
    Drouin Vic
    Posts
    634

    Default

    Find a scrapped forklift tine, good source of thick flat material. I haven't been able to confirm absolutely but I believe they're 4140 or similar. Very hard to find steel of this sort of grade in other than round stock, which would result in a huge amount of waste, whereas a tine will yield a goodly number of toolholders. Economically viable? Depends what you charge yourself per hour.
    Attached Images Attached Images

  3. #3
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    35
    Posts
    1,522

    Default

    There is absolutely no way you could come out ahead financially, the only reasons to make them are if you find the quality of the import holders poor or you need some strange/special holder like anorak bobs special threading holders or a knurler. Cutting the dovetails is a fairly time consuming endeavor as the cutters are very fragile.

  4. #4
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Quote Originally Posted by 19brendan81 View Post
    I am interested in making some home made 250-202 QCTP tool holders. I would be looking to make 3 or 4 of them and was wondering:

    1) Where would I get steel to suit? I think I would need a piece 30mm thick by 90mm wide x 200mm long to make four. I would be able to mill the dovetail in one go with a piece like this.
    For home use almost anything would do. High end industrial units are sometimes ground and hardened but several of us have made holders out of standard black steel and they work well enough.

    Quote Originally Posted by 19brendan81 View Post
    2) Could they be made out of aluminium? I could cast the bar required that way.
    Yes, but unless you know precisely what the composition is and can add the right alloying elements, the cast Al will probably be a bit on the soft side. Drop one and it is likely to be bent. Steel is also lots stronger which if you take heavy cuts is a good thing.

    Quote Originally Posted by 19brendan81 View Post
    3) would this be economically viable given they could be bought new for $45 each delivered? I imagine the steel off the shelf would be very expensive.
    That really depends on what value you put on your time and what else you have on your list. I've bought some, I've made some. With the right set up making is not difficult (one reason I like the Aloris design). The steel would be less than $45 each, especially if you can find some scrap or offcuts at the right price

    If you do go down the homemade route I would suggest while you are set up making up extra dovetailed blanks. The rest is standard milling and having say 4 or 6 blanks sitting in the cupboard for a rainy day is not going to take that much space. I think the record here is someone made a batch of 50 holders. I have from memory 20 or so holders in my lathe cupboard; most have tools in them although I usually swap less common tools around (typically form ground HSS). Remember the whole idea behind a QCTP is that you don't spend time mucking around with adjusting tools, so having commonly used tools set up ready to go (even things like chamfer tools) is preferable.

    Michael

  5. #5
    Join Date
    Oct 2004
    Location
    Southern Highlands NSW
    Posts
    1,898

    Default

    It's nice they are relatively easy to make, when you need a special type that isn't commercially available.

    Jordan

  6. #6
    Join Date
    Apr 2008
    Location
    Canberra
    Posts
    805

    Default

    "Find a scrapped forklift tine"

    Thanks PeteO - that's a great idea. Ill do some ringing around (are there such thing as forklift wreckers???) Did you make the one pictured out of a forklift tine?

    thanks for your thoughts too Michael - re economically viable - I should have explained better - I meant for me to beat the $45 purchase price, not for me to make profit out of them or anything. I'm only interested in doing this for personal consumption so my hourly rate doesn't matter...its all about learning and enjoying being in the shed.

  7. #7
    Join Date
    Apr 2018
    Location
    Drouin Vic
    Posts
    634

    Default

    Quote Originally Posted by 19brendan81 View Post
    "Find a scrapped forklift tine"

    Thanks PeteO - that's a great idea. Ill do some ringing around (are there such thing as forklift wreckers???) Did you make the one pictured out of a forklift tine?

    The holder in the pic I posted is one of a batch I made from part of a forklift tine, they're my go-to source of steel. Tines are scrapped when the heel wears below a specified thickness (they spend a lot of their life dragging on concrete), my scrap metal bloke charges about $60 a pair and usually seems to have a pair or two in the yard.

  8. #8
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    I just bought 8 off 250-202's as i reckon it was almost as cheap. buying the set screws, the nuts, a decent dovetail cutter that may or may not last, and end mill to remove most of the stock for dovetail and tool slot, and then the steel to make..and I was only factoring in old black stuff not machining stuff...and then add my time...nah cheaper to buy and suck on a coldie til they arrive

  9. #9
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Quote Originally Posted by 19brendan81 View Post
    Hi All,

    I am interested in making some home made 250-202 QCTP tool holders. I would be looking to make 3 or 4 of them and was wondering:

    1) Where would I get steel to suit? I think I would need a piece 30mm thick by 90mm wide x 200mm long to make four. I would be able to mill the dovetail in one go with a piece like this.
    2) Could they be made out of aluminium? I could cast the bar required that way.
    3) would this be economically viable given they could be bought new for $45 each delivered? I imagine the steel off the shelf would be very expensive.

    Grateful for any thoughts or suggestions.

    Brendan
    I have the same size commercial QCT blocks on a 12" lathe. They are quite suitable for what I ask them to do.
    I must assume your lathe is around similar size. I wouldn't use aluminium QCTP's for a lathe of that size.

    I say go right ahead. Do it and get it out of your system. You won't be the first or the last of us who has spent $50 making a $10 item.

    We are all making assumptions based upon limited information you have provided so I wouldn't hurt to give us all an idea of the reasons why you want to opt for the DIY route. Is it financial,unavailabe blocks,or you just want a challenging project to do?

    It will be invaluable information for those thinking along similar lines.

    Grahame

  10. #10
    Join Date
    Apr 2008
    Location
    Canberra
    Posts
    805

    Default

    Hi Graham,

    My lathe is a 14 x 40. I want to make them myself for the project, for the flexibility (I have a couple of bespoke designs in mind) and to hopefully save some money. If I can get onto used forks for as cheap as Pete O said I will definitely be able to make them cheaper than $45 each.

    Brendan

  11. #11
    Join Date
    Oct 2011
    Location
    Sydney, NSW
    Posts
    1,249

    Default

    Quote Originally Posted by Pete O View Post
    The holder in the pic I posted is one of a batch I made from part of a forklift tine, they're my go-to source of steel. Tines are scrapped when the heel wears below a specified thickness (they spend a lot of their life dragging on concrete), my scrap metal bloke charges about $60 a pair and usually seems to have a pair or two in the yard.
    We bent a fork tine at work last week (not me - one of the other drivers) which has to be replaced, I might try and get it (or both - I guess they come in pairs?).

    Ben

Similar Threads

  1. Best place to buy spare quick change tool holders from?
    By Com_VC in forum METALWORK GENERAL
    Replies: 18
    Last Post: 9th Dec 2015, 09:31 PM
  2. Replies: 40
    Last Post: 9th Apr 2013, 11:15 PM
  3. quick change tool post help
    By Aerohydro in forum METALWORK GENERAL
    Replies: 5
    Last Post: 23rd Apr 2012, 12:11 AM
  4. quick change tool post
    By scratchbuilt in forum METALWORK GENERAL
    Replies: 18
    Last Post: 13th Mar 2012, 07:46 PM
  5. Quick Change Tool Post
    By tinkera in forum METALWORK GENERAL
    Replies: 3
    Last Post: 22nd Sep 2010, 11:17 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •