does anyone know what the max width and thickness material steel you can bend in a 10 ton press to 45 &90 deg.
does not have to be accurate
thanks steve
-
7th Jul 2018, 11:54 PM #2
You will need to give your vee block die opening first .
Off the top of my head, the rule of thumb was something like 8x thickness so for a 6mm thickness you need a 48mm min die opening.
It is easier to give the material size you hope to bend and calcs can be done on that.
Too many variables the other way - and I have a headache already
Grahame
-
8th Jul 2018, 12:01 AM #3Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,942
Hi Steve, A bit hard to work it out, unless there's a mathematical solution, which I found on Google.
https://sciencing.com/how-8114314-ca...end-metal.html
I'd say at a rough guess about 300mm wide by 3mm thick. The thicker the metal the less width it can do. Probably the max thickness would be about 8mm by 50mm wide, all this would depend on the radius of the die.
I'm no good at maths so I hope this helps,
KrynTo grow old is mandatory, growing up is optional.
-
8th Jul 2018, 12:04 AM #4
Try this link.
Press Brake Tonnage Table from American Machine Tools
Do bear in mind it is imperial dimensions. It took a 10 second search on Google.
Grahame
-
8th Jul 2018, 12:20 AM #5Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,942
Thanks Grahame, just a matter of punching in the correct wording.
KrynTo grow old is mandatory, growing up is optional.
-
8th Jul 2018, 07:50 PM #6Senior Member
- Join Date
- Apr 2014
- Location
- Perth
- Posts
- 134
okay
thanks for the replies
steve
Similar Threads
-
Universal Bender, hand pipe bender, knurling tool, arbor press, chain block
By John T K in forum METALWORK - Machinery, Equipment, MARKETReplies: 12Last Post: 17th Jul 2018, 12:02 AM -
Eye bender Build
By DSEL74 in forum ANTIQUE AND VINTAGE MACHINERYReplies: 5Last Post: 30th Apr 2017, 12:08 AM -
Metal Bender Kit
By SurfinNev in forum METALWORK - Machinery, Equipment, MARKETReplies: 2Last Post: 20th Apr 2017, 08:58 PM -
Rod bender
By Andy Mac in forum METALWORK GENERALReplies: 4Last Post: 4th Aug 2008, 10:47 PM