Lathe from a fire
We had quite a large fire at work. A lathe - https://www.minitech.com.au/lathe-250-x-550-with-g-box - was in a room totally destroyed by the fire. Ceiling is still sitting on top of it at this time. What's the chances of it being scrap from the heat?
Nev.
-
3rd Jul 2018, 08:28 PM #2Senior Member
- Join Date
- Jan 2016
- Location
- Gosford
- Age
- 63
- Posts
- 173
Why are bananas yellow? The question is not going to be easy to answer. Without knowing the intensity of the fire, and how long it was immediately upon the lathe, it's difficult to say. A collapsed ceiling may or may not have done much or any damage more serious than singeing the paint. On the other hand it could have annealed hardened metal and cooked all the wiring. I would assume it's insured so if the insurance company pays out for it, it then belongs to them.
-
3rd Jul 2018, 09:22 PM #3Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,513
Not all bananas are yellow. Anyway, fire was quite intense. Never leave a battery charger switched on, even without a battery in it. Probably the cause of fire according to the fire brigade. Estimated cost to restore power and clean building is $75K.
Nev.
-
3rd Jul 2018, 09:41 PM #4Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
Research what they did in WW2. Plenty of factory fires around then.
Gold, the colour of choice for the discerning person.
-
4th Jul 2018, 06:54 AM #5Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Hi nev. Sorry to hear about the fire. Thats devastating, even if you are insured.
As mentioned, it really is hard to say. The electricals will most likely be cooked, as well as the motor and windings. Anything aluminum like handles etc may have melted. As for the bed, headstock etc, it will depend on how hot it got and how quickly it got cooled down ie with a blast of cold water during F/F operations.
Really tough to say. Most likely id say its a loss but who knows?
Simon
Sent from my SM-G900I using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
4th Jul 2018, 06:15 PM #6Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,513
We got the lathe out today. Much worse than I thought it would be. Total loss. Thought I could maybe get it cheap but not worth the effort.
Nev.
-
4th Jul 2018, 06:18 PM #7Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
I suspected as much.
The ancillary itmes such as chuck, tailstock and steadies my be of some use.
Simon
Sent from my SM-G900I using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
Similar Threads
-
Fire Extinguisher Fun
By RayG in forum METALWORK GENERALReplies: 66Last Post: 14th Nov 2014, 11:05 AM -
help fire damage
By wodstok in forum WELDINGReplies: 6Last Post: 24th Sep 2010, 10:04 PM -
9kg Gas Bottle Barby/Camp Fire
By davmar in forum METALWORK GENERALReplies: 13Last Post: 21st Oct 2008, 08:33 PM -
Can anyone in Adelaide make a fire guard?
By Kaiser Soze in forum METALWORK GENERALReplies: 5Last Post: 11th Feb 2008, 07:43 PM