OT Caustic soda solution lose its potency after it dries out
A while ago I made up a tub of mild paint stripper, 50 litres of water and maybe a kg of 100% NaOH, and used it to remove the paint from 3 or 4 small items. Recently I needed to use the paint stripper again but over time the water had evaporated leaving behind a thick skin of white crystals on the floor of the tub.
Not a problem, refill the tub with water, break up the crystals and stir them back into solution. Put painted item into tub, remove a day later, hose off the paint except that the paint does not budge. The paint hasn't softened or wrinkled it doesn't look too much different to when I put it in the tub.
This is probably not a surprise to the chemists on here, but what has happened to the NaOH?
-
22nd Jun 2018, 07:15 AM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,562
Probably consumed in the chemical reaction the previous time it was used - what you have left is likely not NaOH but a different sodium salt.
For paint stripping these days (and softening hardening brushes too) I use a 50:50 mix of Meths and Turps. Works surprisingly well
Michael
-
22nd Jun 2018, 08:45 AM #3Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
What you have done is scrub CO2 from the air and made sodium carbonate (foot bath salts)
2NaOH(aq) + CO2(g) → Na2CO3(aq) + H2O(l)
-
22nd Jun 2018, 09:38 AM #4Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
What does aq mean?
-
22nd Jun 2018, 10:05 AM #5Senior Member
- Join Date
- Dec 2013
- Location
- Sydney
- Posts
- 201
Aqueous, but what does (l) mean?
-
22nd Jun 2018, 10:18 AM #6Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
It means "in a solution" ie not a solid.
Na2CO3(aq) consists of Na^+ ions and (CO3)^-2 ions and water, same for the NaOH (aq)
This reaction will take place continuously while the water evaporates until the water is gone and all you have left is the Na2Co3
2NaOH(aq) + CO2(g) → Na2CO3(aq) + H2O(l)
Please don't use it as foot bath salts as there could be some residual NaOH present.
BTW the Na2CO3 makes an excellent safe electrolysis salt/
-
22nd Jun 2018, 12:04 PM #7Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
-
22nd Jun 2018, 12:24 PM #8Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Use it to remove rust by electrolysis.
If a carbon rod is used as the other electrode the used solution doesn't go foamy orange and can be safely disposed of down the sewage.
Clean, safe, Na2CO3 costs about $5 for a 500g bag at most supermarkets so it's not worth making it using caustic.
-
10th Jul 2018, 06:48 PM #9Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
Supermarket caustic soda
I've noticed that 500gm packs of supermarket drain cleaner tend to be around 50/50 NaOH and NaCl. Is that to make it work better as a drain cleaner and/or make it cheaper and/or make it less hazardous to the user and/or ???.
-
10th Jul 2018, 07:13 PM #10Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Similar Threads
-
Would like to revisit 'Bicarb Soda Blasting'...........
By KJL1951 aka Kev in forum METALWORK GENERALReplies: 29Last Post: 30th May 2015, 11:22 AM -
Did we lose thread subscriptions in the upgrade?
By marty989 in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACKReplies: 2Last Post: 10th Dec 2012, 12:29 PM -
Best place to buy caustic soda in Adelaide
By nearnexus in forum METALWORK GENERALReplies: 12Last Post: 15th Oct 2012, 01:11 PM -
Granulated Bicarb Soda
By Sterob in forum METALWORK GENERALReplies: 0Last Post: 10th Apr 2011, 01:56 PM -
Soda Blasting
By Sterob in forum METALWORK GENERALReplies: 30Last Post: 24th Jun 2008, 03:34 PM