18th May 2018, 03:22 PM #1Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
Saber split point drill sets
Consolidated Bearings ...CBC picked up these metric 25piece set for $55.00 he didnt have any imperiaks left otherwise i would gave spent more
1526617202422.jpg
Quality looks good.
-
18th May 2018, 06:20 PM #2Banned
- Join Date
- Jan 2018
- Location
- Aldinga Beach.
- Age
- 73
- Posts
- 148
Next time you buy drills try HSS with 5% cobalt. The wife's son bought a set with split points for me when he was living in HK, I won't use anything else now. They never seem to need sharpening, haven't had to sharpen one since the drills arrived.
-
18th May 2018, 06:37 PM #3Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Maybe because you don't use them. All BS aside, the ones with the added Cobalt are an excellent choice.
KrynTo grow old is mandatory, growing up is optional.
-
18th May 2018, 07:43 PM #4Most Valued Member
- Join Date
- Jun 2012
- Location
- SA
- Posts
- 1,649
Are these the same ?
https://adelaidetools.com.au/saber-2...t-10-sbm3.htmlThe worst that can happen is you will fail.
But at least you tried.
-
18th May 2018, 11:47 PM #5Diamond Member
- Join Date
- Oct 2008
- Location
- N.W.Tasmania
- Posts
- 1,407
Those imperiaks are hard to get hold of it seems, and I'm not sure how well they work, but has anyone here tried drills anything like these, https://adelaidetools.com.au/bordo-2...t-2015-m3.html ?
According to the blurb, they are supposed to outperform split point drills, but sharpening them would appear to be a challenge.
Rob.
-
19th May 2018, 11:14 AM #6Banned
- Join Date
- Jan 2018
- Location
- Aldinga Beach.
- Age
- 73
- Posts
- 148
I bought a short set from Aldi with similar points, they perform well. No idea how to re-grind them though.
-
19th May 2018, 01:34 PM #7
That low price for the HSS split points is great.
If you have the need for high production sped there is no contest. There is no advantage for a home DIY guy who drills maybe once a fortnight.
The other factor is that I must be able to sharpen my own drill.
I could not justify the tool and cutter grinder required for such drills.
I have a Tormek wet grinder but it requires a $300 plus jig for drill bit sharpening of split points.
Grahame
Similar Threads
-
Drill point geometry 2
By markgray in forum METALWORK GENERALReplies: 13Last Post: 9th Mar 2017, 11:14 AM -
Torpedos in Split - Any Interest?
By Anorak Bob in forum METALWORK GENERALReplies: 25Last Post: 19th Sep 2014, 09:07 AM -
split roll pins
By morrisman in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 0Last Post: 29th Aug 2014, 08:35 PM -
Split brass bush !
By BaronJ in forum METALWORK GENERALReplies: 19Last Post: 14th Aug 2013, 06:54 AM -
Drill Point Drill
By Penpal in forum METALWORK GENERALReplies: 11Last Post: 18th Jan 2007, 10:22 AM