    Default Water soluble surface plate blue supplier?

    Hi all anyone got a source for water soluble surface plate blue?

    I've tried the blackwoods holti bearing blue and it's inferior to the water based stuff.

  2. #2
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    I didn't even know that water soluble blue was available!

    You can easily make you own to your own specs but it uses oil and prussian blue so it's not water soluble.

    Simon
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  3. #3
    Join Date
    Jun 2008
    Location
    Victoria, Australia
    Age
    74
    Posts
    5,080

    Default

    Quote Originally Posted by j3dprints View Post
    Hi all anyone got a source for water soluble surface plate blue?

    I've tried the blackwoods holti bearing blue and it's inferior to the water based stuff.

    I think you are looking for canode, GregQ bought up a heap and passed it around at one of the scraping classes, he had blue and yellow, some people used both for extra contrast..

    Phil might still have some tubes, if not. This might give you a lead. https://www.artcotools.com/Canode-Bl...tting-Ink.html

  4. #4
    Join Date
    Mar 2017
    Location
    Brisbane
    Posts
    245

    Default

    Yep pretty much canode I think.

    This is what I've found so far I'll post when it gets here if it's any good - https://www.ebay.com.au/itm/Engineer...wAAMXQxzZRfJpj

  5. #5
    Join Date
    May 2012
    Location
    Vermont 3133 Victoria
    Posts
    248

    Default

    G,day,
    l don,t think that one is water soluble. I think Phil had some of that sent to him. I could be wrong though.
    Regards
    Bruce

  6. #6
    Join Date
    Aug 2013
    Location
    Melbourne
    Posts
    229

    Default

    Have a look at ox-tools latest video on YouTube. He talks a bit about water soluble artist supplies for use when scraping, it may be of some use to you.
    Pete

  7. #7
    Join Date
    Aug 2010
    Location
    Near Bendigo, Victoria, AUS
    Age
    72
    Posts
    3,105

    Default

    The eBay link shows a "Marking Blue" - that is for marking out. I doubt that it will work as bearing blue. But I could be wrong and it is a dual purpose blue.... never heard of that before.
    Canode is the only water soluable bearing blue I know of. Will have a look at Oxtools video now.
    Cheers, Joe
    retired - less energy, more time to contemplate projects and more shed time....

  8. #8
    Join Date
    Aug 2013
    Location
    Melbourne
    Posts
    229

    Default

    9D5286CC-1C78-4973-8660-DF7F0E6E0764.pngFrom this weeks 'Monday night meatloaf. Tom Lipton's Oxtools.
    Available from places that sell etching supplies.
    Pete

  9. #9
    Join Date
    Aug 2013
    Location
    Melbourne
    Posts
    229

    Default

    The following mediums are oil based rather than water based, so disregard if it doesn’t suit your needs.

    l have no experience scraping, however a couple of YouTube videos that l found interesting are-
    Wes Johnson, 'Hand scraping how l do it' &
    Brian Ives. 'Hand scraping training video'
    In both these videos they talk about using orange and black cement pigment, mixed with oil to a paste.
    Hope this is of interest to someone.
    Pete

  10. #10
    Join Date
    Jun 2008
    Location
    Victoria, Australia
    Age
    74
    Posts
    5,080

    Default

    9D5286CC-1C78-4973-8660-DF7F0E6E0764.png

    Quote Originally Posted by Petip View Post
    From this weeks 'Monday night meatloaf. Tom Lipton's Oxtools.
    Available from places that sell etching supplies.
    Pete
    That makes sense in a way, the process of making a print from an etching is similiar to marking high spots when scraping. Definately worth further investigation.

    I think it's this stuff https://www.mes.net.au/product-group...762-charbonnel

  11. #11
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    Phil also posted a recipe for making ones own from prussian blu. I have some half dozen blu and red canode and its not as dark as phils recipe. Thus the scrapes dont stand out as well on canode as it does on the prussian blu recipe.

Similar Threads

  1. Looking for a supplier of Dykem Steel Blue
    By RayG in forum METALWORK GENERAL
    Replies: 51
    Last Post: 23rd Oct 2015, 07:03 PM
  2. Surface plate ( granite ) blue
    By morrisman in forum METALWORK GENERAL
    Replies: 14
    Last Post: 2nd Aug 2014, 07:23 PM
  3. shim stock or gauge plate supplier
    By .RC. in forum METALWORK GENERAL
    Replies: 24
    Last Post: 12th Mar 2014, 05:46 PM
  4. what do you think of my surface plate
    By welder in forum METALWORK GENERAL
    Replies: 11
    Last Post: 21st Nov 2011, 05:33 PM
  5. Supplier of Aluminium Chequer Plate in Perth
    By Dan_ms in forum METALWORK GENERAL
    Replies: 2
    Last Post: 11th Apr 2008, 11:25 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •